Removal of cesium ion in aqueous solution using immobilized sericite beads

To apply sericite effectively in the adsorption process, it was immobilized by entrapment method using sodium alginate. Since the immobilized sericite beads have excellent mechanical strength and swelling characteristics, channeling of flow and the increase of pressure drop were not observed through...

Ausführliche Beschreibung

Gespeichert in:
Bibliographische Detailangaben
Veröffentlicht in:The Korean journal of chemical engineering 2014, 31(7), 172, pp.1219-1224
Hauptverfasser: Jeon, Choong, Kim, Jong-Oh, Lee, Seung-Mok
Format: Artikel
Sprache:eng
Schlagworte:
Online-Zugang:Volltext
Tags: Tag hinzufügen
Keine Tags, Fügen Sie den ersten Tag hinzu!
Beschreibung
Zusammenfassung:To apply sericite effectively in the adsorption process, it was immobilized by entrapment method using sodium alginate. Since the immobilized sericite beads have excellent mechanical strength and swelling characteristics, channeling of flow and the increase of pressure drop were not observed through column operations. In addition, it was also stable under pH 10 and 45 °C of cesium solution. The maximum adsorption capacity and Langmuir adsorption constant was 1.430mg/g and 2.329 L/mg, respectively, at initial pH 5 of cesium solution in batch type and the Langmuir model with higher correlation coefficient of 0.997 fits experimental data better than Freundlich model. The breakthrough point emerged around 15 (1.0 mL/min) and 20 bed volumes (0.5 mL/min), and the cesium ions bound to the immobilized sericite beads were readily released and quantitatively recovered by a few bed volumes of 1.0M of HNO 3 solution. Furthermore, bed volumes of cesium ions for firstly reused sericite beads can be still maintained as 18, which shows good regeneration ability.
ISSN:0256-1115
1975-7220
DOI:10.1007/s11814-014-0058-7