Low swelling poly(ester) urethane composite containing modified hollow glass microspheres for seawater-resistant encapsulant
A novel poly(ester) urethane system filled with poly(ester) urethane grafted with hollow glass microspheres was fabricated via a melt mixing method for use as an underwater encapsulant. The poly(ester) urethane/ poly(ester) urethane grafted with hollow glass microsphere (HGM) composites (PU/PU- g -H...
Gespeichert in:
Veröffentlicht in: | Macromolecular research 2012, 20(12), , pp.1271-1280 |
---|---|
Hauptverfasser: | , , , |
Format: | Artikel |
Sprache: | eng |
Schlagworte: | |
Online-Zugang: | Volltext |
Tags: |
Tag hinzufügen
Keine Tags, Fügen Sie den ersten Tag hinzu!
|
Zusammenfassung: | A novel poly(ester) urethane system filled with poly(ester) urethane grafted with hollow glass microspheres was fabricated
via
a melt mixing method for use as an underwater encapsulant. The poly(ester) urethane/ poly(ester) urethane grafted with hollow glass microsphere (HGM) composites (PU/PU-
g
-HGM composites) were prepared using various PU
-g-
HGM contents. Studies of these composites showed that the swelling ratio of PU/PU
g
-HGM composites in seawater and paraffin oil decreased with increasing HGM content of grafted poly(ester) urethane, while the tensile strength of PU/PU-
g
-HGM composites could be incrementally increased by rising PU-
g
-HGM content. This finding is due to the enhanced interfacial adhesion between poly(ester) urethane and poly(ester) urethane-grafted HGM due to good compatibility between these components. The tensile strength of the PU/PU-
g
-HGM composites in seawater (or paraffin oil) also exhibited higher levels than those of poly(ester) urethane and PU/ pristine HGMs composites in seawater (or paraffin oil) as the immersion time increased. Therefore, the PU/PU-
g
-HGM composites were expected to have potential applications as underwater encapsulants. |
---|---|