의치 세정제가 탄성 의치상 이장재에 미치는 효과에 관한 연구

To determine the compatibilities of soft liming materials with denture cleansers by measuring the flexibility and elasticity and investigating the surface changes, 4 self-curing acrylic resin soft lining materials and 1 heat-curing silicone soft lining material were evaluated. 3mm thick x 20mm diame...

Ausführliche Beschreibung

Gespeichert in:
Bibliographische Detailangaben
Veröffentlicht in:Taehan Chikwa Poch'ol Hakhoe chi 1993, Vol.31 (2), p.219-235
Hauptverfasser: 장복숙, 김창회, 김영수, Jang, Bok-Sook, Kim, Chang-Whe, Kim, Yung-Soo
Format: Artikel
Sprache:kor
Online-Zugang:Volltext
Tags: Tag hinzufügen
Keine Tags, Fügen Sie den ersten Tag hinzu!
Beschreibung
Zusammenfassung:To determine the compatibilities of soft liming materials with denture cleansers by measuring the flexibility and elasticity and investigating the surface changes, 4 self-curing acrylic resin soft lining materials and 1 heat-curing silicone soft lining material were evaluated. 3mm thick x 20mm diameter discs of soft lining materials were individually bonded to a hard acrylic resin base as per manufacturers’instructions. Using an Instron universal testing machine, a static stress of $2kg/cm^2$ was applied for 30secs., the strain in compression was measured, giving an indication of the material’s flexibility. Elastic recovery was measured at 10secs. After removal of stress. Surface changes were investigated with Stereomicroscope. Then the specimens were immersed in 4alkaline peroxide denture cleansers and water as control group, tests were carried out at 1 day, 2 days, 7 days, 14 days and 30 days. The results were as follows : 1. Alkaline peroxide denture cleansers caused considerable porosity on the surface of selfcuring acrylic resin soft lining materials, and the most affected by the cleansers were Viscogel, Coe-Soft, Coe-Comfort, Lynal, in that order. 2. There was significant difference in flexibility between each soft lining material except for Coe-Comfort and Visco-gel, and every soft lining material was significant difference in elasticity. Especially Molloplast-B and Lynal were less flexible and more elastic than other soft lining materials(p
ISSN:0301-2875