Magnetic Properties of Ternary Fe-Ni-Ti Alloys After Severe Plastic Deformation

We report on magnetic properties of Fe-Ni-Ti alloys after severe plastic deformation (SPD) by high-pressure torsion (HPT) and low-temperature annealing. SPD and low-temperature annealing considerably change the magnetization behavior. The main magnetic and structural characteristics of bulk and HPT...

Ausführliche Beschreibung

Gespeichert in:
Bibliographische Detailangaben
Veröffentlicht in:IEEE magnetics letters 2020, Vol.11, p.1-4
Hauptverfasser: Taskaev, Sergey V., Ulyanov, Maxim N., Gunderov, Dmitriy V., Bogush, Mikhail Yu
Format: Artikel
Sprache:eng
Schlagworte:
Online-Zugang:Volltext bestellen
Tags: Tag hinzufügen
Keine Tags, Fügen Sie den ersten Tag hinzu!
Beschreibung
Zusammenfassung:We report on magnetic properties of Fe-Ni-Ti alloys after severe plastic deformation (SPD) by high-pressure torsion (HPT) and low-temperature annealing. SPD and low-temperature annealing considerably change the magnetization behavior. The main magnetic and structural characteristics of bulk and HPT materials were determined. The addition of small amounts of Ti and annealing at 300 °C will not lead to the formation of the L1 0 structure even with the use of the SPD technique.