Preferable opening area of screen mesh to print fine finger electrode with less-bumpy surface
It is important to select suitable screen mask for printing fine electrode. In case of fine line printing with 50 μm width, we demonstrated that the screen mask with 39% opening is the best selection compared with 49% and 60% opening. Variation (max and min) of width and thickness of fine electrode...
Gespeichert in:
Hauptverfasser: | , , , , , |
---|---|
Format: | Tagungsbericht |
Sprache: | eng |
Schlagworte: | |
Online-Zugang: | Volltext bestellen |
Tags: |
Tag hinzufügen
Keine Tags, Fügen Sie den ersten Tag hinzu!
|
Zusammenfassung: | It is important to select suitable screen mask for printing fine electrode. In case of fine line printing with 50 μm width, we demonstrated that the screen mask with 39% opening is the best selection compared with 49% and 60% opening. Variation (max and min) of width and thickness of fine electrode shows lower value when using low opening rate. |
---|---|