Fabricating of Lithium-Battery-Grade Precursor Salt Cobaltous Carbonate
Some factors affect precursor capability, for example: raw material CoCl 2 solution impurity, feeding methods of reactants, solutions' pH value of deposition reaction, washing conditions, etc. Cobalt chloride is chosen as raw material, sodium carbonate as precipitator, cobalt ion concentration...
Gespeichert in:
Hauptverfasser: | , , , |
---|---|
Format: | Tagungsbericht |
Sprache: | eng |
Schlagworte: | |
Online-Zugang: | Volltext bestellen |
Tags: |
Tag hinzufügen
Keine Tags, Fügen Sie den ersten Tag hinzu!
|
Zusammenfassung: | Some factors affect precursor capability, for example: raw material CoCl 2 solution impurity, feeding methods of reactants, solutions' pH value of deposition reaction, washing conditions, etc. Cobalt chloride is chosen as raw material, sodium carbonate as precipitator, cobalt ion concentration 65~70g/L, Cobalt chloride/sodium carbonate(mol ratio)among 0.63~0.72, the way adding solution is chosen that precipitator is added to cobalt chloride solution, precipitated pH is chosen among 9.0~9.5. Under such conditions, better precursor can be acquired. |
---|---|
DOI: | 10.1109/ICICTA.2010.25 |