Originality method in selecting high CTE molding underfill for low profile molded FCCSP

In this paper, we propose a originality method in selecting high CTE molding underfill to control the warpage of low profile molded FCCSP with 0.8 mm package height. A test vehicle was designed with package size of 7.5 × 7.5 mm and die size 6.5 × 5.9 mm with 65 nm low K chip, the package height is 0...

Ausführliche Beschreibung

Gespeichert in:
Bibliographische Detailangaben
Hauptverfasser: HuiMin Huang, ChinNan Lin, HoYi Tsai, YihJenn Jiang, Chiu, S.
Format: Tagungsbericht
Sprache:eng
Schlagworte:
Online-Zugang:Volltext bestellen
Tags: Tag hinzufügen
Keine Tags, Fügen Sie den ersten Tag hinzu!
Beschreibung
Zusammenfassung:In this paper, we propose a originality method in selecting high CTE molding underfill to control the warpage of low profile molded FCCSP with 0.8 mm package height. A test vehicle was designed with package size of 7.5 × 7.5 mm and die size 6.5 × 5.9 mm with 65 nm low K chip, the package height is 0.8 mm after solder ball reflow, total IO count is 196 (Figure 1). We will demonstrate the warpage comparison of normal CTE (10~12) & high CTE (>12) molding underfill and the reliability test results. In this study, the experiment result can achieve our expectation which warpage is less than 3mil and the reliability had passed MSL3 (Moisture Sensitivity Test, 60°C/60% ,40 hours + 3 times of IR260°C.), TCT (Temperature cycling test, -55 ~ 125.) 1500 cycles, HAST (High accelerated stress test, 130~C/85% R.H) 100 hours, TST (Thermal shock test, -55 ~ 125°C) 500 cycles and HTSL (High temperature storage life, 150°C) 1000 hours.