Abrasive waterjet (AWJ) titanium tangential turning evaluation

The paper deals with abrasive waterjet titanium tangential turning. Titanium grade 3 with a diameter of 55 mm was used as an experimental material. Technological conditions of turning tests were the same by gradually changing value of traverse speed (vf = 1,5; 3; 4,5; 6; 7,5 mm・min-1). Experiment te...

Ausführliche Beschreibung

Gespeichert in:
Bibliographische Detailangaben
Veröffentlicht in:Metalurgija 2014-10, Vol.53 (4), p.537
Hauptverfasser: Hloch, S, Hlaváček, J, Vasilko, K, Cárach, J, Samardžić, I, Kozak, D, Hlavatý, I, Ščučka, J. J, Klich, J, Klichová, D
Format: Artikel
Sprache:eng
Schlagworte:
Online-Zugang:Volltext
Tags: Tag hinzufügen
Keine Tags, Fügen Sie den ersten Tag hinzu!
Beschreibung
Zusammenfassung:The paper deals with abrasive waterjet titanium tangential turning. Titanium grade 3 with a diameter of 55 mm was used as an experimental material. Technological conditions of turning tests were the same by gradually changing value of traverse speed (vf = 1,5; 3; 4,5; 6; 7,5 mm・min-1). Experiment tests were performed by using continuous abrasive waterjet of pressure p = 400MPa, by rotation n = 60 rpm of workpiece. The abrasive particles (Barton Garnet) were fed to the waterjet in the amount of 0,4 kg・min-1. It was determined that acceleration of traverse speed did not increase the surface profile parameters.