Low Temperature Oxidation of Pure Iron: Growth Kinetics and Scale Morphologies

Isothermal oxidation of pure iron has been performed in air at atmospheric pressure between 260°C and 500°C. Growth kinetics are accurately analysed and scale morphologies are investigated by SEM and TEM observations. The calculation of the variations of the parabolic rate constant kp with scale thi...

Ausführliche Beschreibung

Gespeichert in:
Bibliographische Detailangaben
Veröffentlicht in:Materials science forum 2004-01, Vol.461-464, p.591-598
Hauptverfasser: Monceau, Daniel, Bertrand, Nathalie, Gauvain, Danielle, Desgranges, Clara, Poquillon, Dominique
Format: Artikel
Sprache:eng
Schlagworte:
Online-Zugang:Volltext
Tags: Tag hinzufügen
Keine Tags, Fügen Sie den ersten Tag hinzu!
Beschreibung
Zusammenfassung:Isothermal oxidation of pure iron has been performed in air at atmospheric pressure between 260°C and 500°C. Growth kinetics are accurately analysed and scale morphologies are investigated by SEM and TEM observations. The calculation of the variations of the parabolic rate constant kp with scale thickness allows a better understanding of scale growth mechanisms involved at this intermediate temperature range, which have been poorly investigated up to now. These results are discussed with the objective of long term behaviour for long term interim storage of some nuclear waste containers.
ISSN:0255-5476
1662-9752
1662-9752
1662-9760
DOI:10.4028/www.scientific.net/MSF.461-464.591