Thermal cycling creep properties of a directionally solidified superalloy DZ125

Aero-engine turbine blades may suffer overheating during service, which can result in severe microstructural and mechanical degradation within tens of seconds. In this study, the thermal cycling creep under (950 °C/15 min+1100 °C/1 min)-100 MPa was performed on a directionally solidified superalloy,...

Ausführliche Beschreibung

Gespeichert in:
Bibliographische Detailangaben
Veröffentlicht in:Journal of materials science & technology 2022-03, Vol.104, p.269-284
Hauptverfasser: An, Wenrui, Utada, Satoshi, Guo, Xiaotong, Antonov, Stoichko, Zheng, Weiwei, Cormier, Jonathan, Feng, Qiang
Format: Artikel
Sprache:eng
Schlagworte:
Online-Zugang:Volltext
Tags: Tag hinzufügen
Keine Tags, Fügen Sie den ersten Tag hinzu!
Beschreibung
Zusammenfassung:Aero-engine turbine blades may suffer overheating during service, which can result in severe microstructural and mechanical degradation within tens of seconds. In this study, the thermal cycling creep under (950 °C/15 min+1100 °C/1 min)-100 MPa was performed on a directionally solidified superalloy, DZ125. The effects of overheating and thermal cycling on the creep properties were evaluated in terms of creep behavior and microstructural evolution against isothermally crept specimens under 950 °C/100 MPa, 950 °C/270 MPa, and 1100 °C/100 MPa. The results indicated that the thermal cycling creep life was reduced dramatically compared to the isothermal creep under 950 °C/100 MPa. The plastic creep deformation mainly occurred during the overheating stage during the thermal cycling creep. The thermal cycling creep curve exhibited three stages, similar to the 1100 °C isothermal creep, but its minimum creep rate occurred at a lower creep strain. The overheating events caused severe microstructural degradation, such as substantial dissolution of γ' phase, earlier formation of rafted γ' microstructure, widening of the γ channels, and instability of the interfacial dislocation networks. This microstructural degradation was the main reason for the dramatic decrease in thermal cycling creep life, as the thermal cycling promoted more dislocations to cut into γ' phase and more cracks to initiate at grain boundaries, carbides, and residual eutectic pools. This study underlines the importance of evaluating the thermal cycling creep properties of superalloys to be used as turbine blades and provides insights into the effect of thermal cycling on directionally solidified superalloys for component design. •The thermal cycling creep was conducted on a directionally solidified superalloy to simulate the overheating service condition of turbine blades.•The thermal cycling promoted more dislocations to cut into γ' phase, leading to the earlier occurrence of the minimum creep rate compare with the isothermal creep.•Dramatic decrease of the thermal cycling creep life was due to the severe microstructural degradation during overheating such as γ' phase dissolution, γ channel widening, and dislocation networks instability.•The thermal cycling promoted more cracks to initiate at the weak regions such as grain boundaries, carbides, and residual eutectic pools. [Display omitted]
ISSN:1005-0302
1941-1162
DOI:10.1016/j.jmst.2021.07.015