Synthesis process of nanowired Al/CuO thermite

Al/CuO nanothermites were fabricated by thermal oxidation of copper layer at 450 °C for 5 h and by aluminum thermal evaporation: thermal evaporation allows producing thin layer less than 2 μm in size. The copper has been deposited by electroplating or thermal evaporation depending on the required th...

Ausführliche Beschreibung

Gespeichert in:
Bibliographische Detailangaben
Veröffentlicht in:The Journal of physics and chemistry of solids 2010-02, Vol.71 (2), p.80-83
Hauptverfasser: Petrantoni, M., Rossi, C., Conédéra, V., Bourrier, D., Alphonse, P., Tenailleau, C.
Format: Artikel
Sprache:eng
Schlagworte:
Online-Zugang:Volltext
Tags: Tag hinzufügen
Keine Tags, Fügen Sie den ersten Tag hinzu!
Beschreibung
Zusammenfassung:Al/CuO nanothermites were fabricated by thermal oxidation of copper layer at 450 °C for 5 h and by aluminum thermal evaporation: thermal evaporation allows producing thin layer less than 2 μm in size. The copper has been deposited by electroplating or thermal evaporation depending on the required thickness. The obtained diameter of Al/CuO nanowires is 150–250 nm. Al/CuO nanowires composite were characterized by scanning electron microscopy (SEM), X-ray diffraction (XRD), differential scanning calorimetry (DSC) and differential thermal analysis (DTA). Two distinct exothermic reactions occurred at 515 and 667 °C and total energy release of this thermite is 10 kJ/cm 3.
ISSN:0022-3697
1879-2553
DOI:10.1016/j.jpcs.2009.07.020