Deterioration data of a large-scale reinforced concrete specimen with severe ASR/DEF deterioration

[Display omitted] •A large-scale RC specimen is subjected to ASR/DEF deterioration for five years.•Crack widths of up to 30mm measured; rebars yield within one year of exposure.•Transverse strains exceed longitudinal strains due to low transverse steel content.•Surface expansion strains closely rela...

Ausführliche Beschreibung

Gespeichert in:
Bibliographische Detailangaben
Veröffentlicht in:Construction & building materials 2016-10, Vol.124, p.20-30
Hauptverfasser: Karthik, Madhu M., Mander, John B., Hurlebaus, Stefan
Format: Artikel
Sprache:eng
Schlagworte:
Online-Zugang:Volltext
Tags: Tag hinzufügen
Keine Tags, Fügen Sie den ersten Tag hinzu!
Beschreibung
Zusammenfassung:[Display omitted] •A large-scale RC specimen is subjected to ASR/DEF deterioration for five years.•Crack widths of up to 30mm measured; rebars yield within one year of exposure.•Transverse strains exceed longitudinal strains due to low transverse steel content.•Surface expansion strains closely relate to the local reinforcement layout.•Surface strains compare well with internal steel and concrete gauge strain measurements. Limited field data are available from reinforced concrete specimens exposed to environmental conditions and subjected to severe deterioration by Alkali Silica Reaction (ASR) and/or Delayed Ettringite Formation (DEF). A large-scale reinforced concrete specimen is subject to ASR/DEF deterioration for five years. Strain measurements indicate that both transverse and longitudinal reinforcement yield within six to twelve months of field exposure. Recorded surface strains compare well with the internal steel and concrete strains. Transverse expansion strains markedly exceed longitudinal expansion strains. Although ASR/DEF deterioration may cause severe surface cracking and possible reinforcement corrosion in the long-term, its effect on the structure’s load carrying capacity remains unknown at this time.