Nordic Pulp & Paper Research Journal

This review covers the effect of mechanical pre-treatment of wood chips on the energy consumption in refining and the quality of pulp. To understand the mechanisms of mechanical pre-treatment, a short description of relevant refining theory and reported effects of pre-treatment on wood morphology is...

Ausführliche Beschreibung

Gespeichert in:
Bibliographische Detailangaben
Hauptverfasser: Gorski Dmitri , Mittuniversitetet, Institutionen för naturvetenskap, teknik och matematik, Hill J, Engstrand Per , Mittuniversitetet, Institutionen för naturvetenskap, teknik och matematik, Engstrand Per, Mittuniversitet, Department of Science, Technology and Mathematics, Johansson Lars
Format: Web Resource
Sprache:eng ; swe
Online-Zugang:Volltext bestellen
Tags: Tag hinzufügen
Keine Tags, Fügen Sie den ersten Tag hinzu!
Beschreibung
Zusammenfassung:This review covers the effect of mechanical pre-treatment of wood chips on the energy consumption in refining and the quality of pulp. To understand the mechanisms of mechanical pre-treatment, a short description of relevant refining theory and reported effects of pre-treatment on wood morphology is given. Mechanical pre-treatment offers a chance to utilize the energy needed to defibrate chips in a more efficient way, minimizing the cyclic elastic deformations which are the main defibration mechanism in refining. Studies of fibre morphology indicate that compressive pretreatment mechanically introduces favorable weak points in the S1 and S2 fibre walls where defibration proceeds easier upon subsequent refining.Published results which cover the effect of the pretreatment on energy consumption and pulp properties are reviewed. Energy reduction of between 10% and 30% is reported in the literature. High ratio of volumetric compression is necessary. Pressurized conditions are required to ensure that the fibres are not damaged during the pre-treatment. Other effects of compressive pretreatment include a more uniform chip size and moisture content, better penetration of chemicals and removal of extractives from the chips. A list of equipment used for chip pre-compression is provided together with published results of pilot-scale and mill-scale operation. Published This review covers the effect of mechanical pre-treatment of wood chips on the energy consumption in refining and the quality of pulp. To understand the mechanisms of mechanical pre-treatment, a short description of relevant refining theory and reported effects of pre-treatment on wood morphology is given. Mechanical pre-treatment offers a chance to utilize the energy needed to defibrate chips in a more efficient way, minimizing the cyclic elastic deformations which are the main defibration mechanism in refining. Studies of fibre morphology indicate that compressive pretreatment mechanically introduces favorable weak points in the S1 and S2 fibre walls where defibration proceeds easier upon subsequent refining.Published results which cover the effect of the pretreatment on energy consumption and pulp properties are reviewed. Energy reduction of between 10% and 30% is reported in the literature. High ratio of volumetric compression is necessary. Pressurized conditions are required to ensure that the fibres are not damaged during the pre-treatment. Other effects of compressive pretreatment include a more