Segmented copolymers their manufacture and blends with polypropylene
Segmented copolymers of polypropylene with stryene, when made using an initiator having a one-hour half life at a temperature of 110 to 125 DEG C in a process involving a heating rate of at least 1 DEG C per minute, are desirable sag-resistance improvers for polyproplyene.