POSTTREATED PROSTHETIC DEVICE
An improved process for manufacturing a molded prosthetic device from a synthetic bioabsorbable polymer is disclosed. The process includes placing a solid amount of the polymer in a molding machine; melting the polymer by subjecting it to a temperature of from about 240 DEG to 255 DEG C. for about 2...
Gespeichert in:
Hauptverfasser: | , |
---|---|
Format: | Patent |
Sprache: | eng |
Schlagworte: | |
Online-Zugang: | Volltext bestellen |
Tags: |
Tag hinzufügen
Keine Tags, Fügen Sie den ersten Tag hinzu!
|
Zusammenfassung: | An improved process for manufacturing a molded prosthetic device from a synthetic bioabsorbable polymer is disclosed. The process includes placing a solid amount of the polymer in a molding machine; melting the polymer by subjecting it to a temperature of from about 240 DEG to 255 DEG C. for about 2 to 5 minutes; transporting the polymer melt to an orifice; injecting the polymer melt from the orifice into a closed mold cavity at a pressure of from about 8000 to 9000 lbs per square inch (562 to 633 kg per sq. cm.); holding the polymer in the mold cavity for less than about one minute at a temperature of about 70 DEG to 90 DEG C.; removing a molded prosthetic device from the mold cavity; and posttreating the molded prosthetic device. The posttreating can be, e.g., annealing and then/or sterilizing. |
---|