METHOD FOR BREAKING DOWN A MIXTURE OF SOLID PARTICLES COMPRISING RUTHENIUM

A method for breaking down a mixture, which is present in the form of solid particles, consisting of: (A) 0 to 99% by weight of metallic ruthenium, (B) 0 to 50% by weight of at least one element other than ruthenium, which is present in elementary form, selected from the group of elements of the ato...

Ausführliche Beschreibung

Gespeichert in:
Bibliographische Detailangaben
Hauptverfasser: GÜNTHER, Magdalena, KRÖCKEL, Sophia, STETTNER, Martin
Format: Patent
Sprache:eng
Online-Zugang:Volltext bestellen
Tags: Tag hinzufügen
Keine Tags, Fügen Sie den ersten Tag hinzu!
Beschreibung
Zusammenfassung:A method for breaking down a mixture, which is present in the form of solid particles, consisting of: (A) 0 to 99% by weight of metallic ruthenium, (B) 0 to 50% by weight of at least one element other than ruthenium, which is present in elementary form, selected from the group of elements of the atomic numbers 13, 21-30, 39-42, 45-52, and 72-83, (C) 0 to 99% by weight of ruthenium oxide, (D) 0 to 70% by weight of at least one solid element oxide other than ruthenium, (E) 0 to 30% by weight of at least one inorganic substance other than (A) to (D), and (F) 0 to 3% by weight of at least one organic substance, wherein the sum of the % by weight of the compounds (A) to (F) is 100% by weight and the ruthenium content of the mixture is 2 to 99% by weight, and wherein the method comprises the steps of: (1) optionally mixing said mixture with alkali carbonate by forming a blend, (2) alkaline oxidizing breakdown of the mixture or of the blend, respectively, formed in optional step (1) into molten potassium hydroxide using a gaseous oxidizing agent selected from the group consisting of air, oxygen, and air/oxygen mixtures, and without use of nitrate, and (3) cooling down the breakdown material formed in step (2) to a temperature below its solidification temperature, wherein the gaseous oxidizing agent is introduced into the melt in step (2).