PROCESS FOR PREPARING SELF-DISINTEGRATING DICALCIUM SILICATE OR PRODUCTS CONTAINING SUCH A MATERIAL

To the starting material containing at least 10 percent of SiO2 and 25 percent of Al2O3, limestone and small quantities of metallic desoxidants are admixed, and having been clinkerized at a temperature of 1,250 DEG to 1,420 DEG C it is cooled abruptly with air and/or water to a temperature of about...

Ausführliche Beschreibung

Gespeichert in:
Bibliographische Detailangaben
Hauptverfasser: GALAUNER BELA, LAZAR FERENC, KAPOLYI LASZLO, VAMOS GYOERGY
Format: Patent
Sprache:eng
Schlagworte:
Online-Zugang:Volltext bestellen
Tags: Tag hinzufügen
Keine Tags, Fügen Sie den ersten Tag hinzu!
Beschreibung
Zusammenfassung:To the starting material containing at least 10 percent of SiO2 and 25 percent of Al2O3, limestone and small quantities of metallic desoxidants are admixed, and having been clinkerized at a temperature of 1,250 DEG to 1,420 DEG C it is cooled abruptly with air and/or water to a temperature of about 700 DEG C. The extracted product can be used for alumina production, the residue for cement production.