METAL AND FLUORINE VALUES RECOVERY FROM MINERAL ORE TREATMENT
The process for recovering Ta/Nb values from highly fluorinated ore materials by the process of: (a) contacting the materials with one or a mixture of HNO3 or HC1, and H3BO3 wherein the H3BO3 to other acid molar ratio is from about 1/10 to about 1/1, (b) maintaining the temperature between about 55...
Gespeichert in:
1. Verfasser: | |
---|---|
Format: | Patent |
Sprache: | eng ; fre |
Schlagworte: | |
Online-Zugang: | Volltext bestellen |
Tags: |
Tag hinzufügen
Keine Tags, Fügen Sie den ersten Tag hinzu!
|
Zusammenfassung: | The process for recovering Ta/Nb values from highly fluorinated ore materials by the process of: (a) contacting the materials with one or a mixture of HNO3 or HC1, and H3BO3 wherein the H3BO3 to other acid molar ratio is from about 1/10 to about 1/1, (b) maintaining the temperature between about 55 DEG C and about 85 DEG C, (c) reacting for a sufficient period to substantially solubilize the major portion of the materials and to substantially insolubilize all Ta/Nb values, and (d) separating the solids containing the Ta/Nb values from solution.
Le procédé de récupération de Ta/Nb à partir de minerais hautement fluorés consiste à: (a) mettre en contact le minerai avec du HNO3 ou du HC1 (ou un mélange des deux), ainsi que du H3BO3, le rapport molaire du H3BO3 aux autres acides étant dans la plage allant de 1/10 environ à 1/1 environ, (b) maintenir la température entre 55 DEG C environ et 85 DEG C environ, (c) laisser se faire la réaction pendant une durée suffisante pour rendre soluble la majeure partie du minerai et pour rendre insoluble pratiquement tout le Ta/Nb, et (d) à séparer de la solution les matières solides contenant le Ta/Nb. |
---|