THERMALLY ANNEALED GRATINGS IN COATED FIBER AND RELATED SYSTEMS AND METHODS

Described herein are systems, methods, and articles of manufacture for a coated fiber modified by actinic radiation to increase back-scattering, which experiences very little back scattering decay at a temperature and time of exposure that is sufficient to noticeably degrade the coating and/or notic...

Ausführliche Beschreibung

Gespeichert in:
Bibliographische Detailangaben
Hauptverfasser: DYER, Robert, SAVRAN, Brian, STOLOV, Andrei, WESTBROOK, Paul, SOUNDARA, Vixay, HOKANSSON, Adam, POPELKA, Matthew
Format: Patent
Sprache:eng ; fre
Schlagworte:
Online-Zugang:Volltext bestellen
Tags: Tag hinzufügen
Keine Tags, Fügen Sie den ersten Tag hinzu!
container_end_page
container_issue
container_start_page
container_title
container_volume
creator DYER, Robert
SAVRAN, Brian
STOLOV, Andrei
WESTBROOK, Paul
SOUNDARA, Vixay
HOKANSSON, Adam
POPELKA, Matthew
description Described herein are systems, methods, and articles of manufacture for a coated fiber modified by actinic radiation to increase back-scattering, which experiences very little back scattering decay at a temperature and time of exposure that is sufficient to noticeably degrade the coating and/or noticeably degrade the optical fiber due to outgassing of hydrogen from the coating, wherein an optical fiber comprises a fiber length, a coating having a treated coating weight, wherein the treated coating weight is at least 25% less of an original coating weight prior to an annealing treatment, and an optical back-scatter along the fiber length greater than a Rayleigh back-scattering over the fiber length, wherein the optical back-scatter does not decrease along the fiber length by more than 3 dB after exposure to annealing treatment. L'invention concerne des systèmes, des procédés, et des articles de fabrication pour une fibre revêtue modifiée par un rayonnement actinique pour augmenter la rétrodiffusion, qui subit une très faible décroissance de la rétrodiffusion à une température et un temps d'exposition qui est suffisant pour dégrader sensiblement le revêtement et/ou dégrader sensiblement la fibre optique due au dégazage de l'hydrogène du revêtement, une fibre optique comprenant une longueur de fibre, un revêtement ayant un poids de revêtement traité, le poids de revêtement traité étant d'au moins 25 % inférieur à un poids de revêtement d'origine avant un traitement de recuit, et une rétrodiffusion optique le long de la longueur de fibre supérieure à une rétrodiffusion de Rayleigh sur la longueur de la fibre, la rétrodiffusion optique ne diminuant pas le long de la longueur de fibre de plus de 3 dB après exposition à un traitement de recuit.
format Patent
fullrecord <record><control><sourceid>epo_EVB</sourceid><recordid>TN_cdi_epo_espacenet_WO2022169902A1</recordid><sourceformat>XML</sourceformat><sourcesystem>PC</sourcesystem><sourcerecordid>WO2022169902A1</sourcerecordid><originalsourceid>FETCH-epo_espacenet_WO2022169902A13</originalsourceid><addsrcrecordid>eNrjZPAO8XAN8nX08YlUcPTzc3X0cXVRcA9yDPH0cw9W8PRTcPZ3DAEKuXk6uQYBVbgoBLn6gEWCI4NDXH2DwWK-riEe_i7BPAysaYk5xam8UJqbQdnNNcTZQze1ID8-tbggMTk1L7UkPtzfyMDIyNDM0tLAyNHQmDhVAB-xLk8</addsrcrecordid><sourcetype>Open Access Repository</sourcetype><iscdi>true</iscdi><recordtype>patent</recordtype></control><display><type>patent</type><title>THERMALLY ANNEALED GRATINGS IN COATED FIBER AND RELATED SYSTEMS AND METHODS</title><source>esp@cenet</source><creator>DYER, Robert ; SAVRAN, Brian ; STOLOV, Andrei ; WESTBROOK, Paul ; SOUNDARA, Vixay ; HOKANSSON, Adam ; POPELKA, Matthew</creator><creatorcontrib>DYER, Robert ; SAVRAN, Brian ; STOLOV, Andrei ; WESTBROOK, Paul ; SOUNDARA, Vixay ; HOKANSSON, Adam ; POPELKA, Matthew</creatorcontrib><description>Described herein are systems, methods, and articles of manufacture for a coated fiber modified by actinic radiation to increase back-scattering, which experiences very little back scattering decay at a temperature and time of exposure that is sufficient to noticeably degrade the coating and/or noticeably degrade the optical fiber due to outgassing of hydrogen from the coating, wherein an optical fiber comprises a fiber length, a coating having a treated coating weight, wherein the treated coating weight is at least 25% less of an original coating weight prior to an annealing treatment, and an optical back-scatter along the fiber length greater than a Rayleigh back-scattering over the fiber length, wherein the optical back-scatter does not decrease along the fiber length by more than 3 dB after exposure to annealing treatment. L'invention concerne des systèmes, des procédés, et des articles de fabrication pour une fibre revêtue modifiée par un rayonnement actinique pour augmenter la rétrodiffusion, qui subit une très faible décroissance de la rétrodiffusion à une température et un temps d'exposition qui est suffisant pour dégrader sensiblement le revêtement et/ou dégrader sensiblement la fibre optique due au dégazage de l'hydrogène du revêtement, une fibre optique comprenant une longueur de fibre, un revêtement ayant un poids de revêtement traité, le poids de revêtement traité étant d'au moins 25 % inférieur à un poids de revêtement d'origine avant un traitement de recuit, et une rétrodiffusion optique le long de la longueur de fibre supérieure à une rétrodiffusion de Rayleigh sur la longueur de la fibre, la rétrodiffusion optique ne diminuant pas le long de la longueur de fibre de plus de 3 dB après exposition à un traitement de recuit.</description><language>eng ; fre</language><subject>CHEMICAL COMPOSITION OF GLASSES, GLAZES, OR VITREOUSENAMELS ; CHEMISTRY ; GLASS ; JOINING GLASS TO GLASS OR OTHER MATERIALS ; MANUFACTURE, SHAPING, OR SUPPLEMENTARY PROCESSES ; METALLURGY ; MINERAL OR SLAG WOOL ; OPTICAL ELEMENTS, SYSTEMS, OR APPARATUS ; OPTICS ; PHYSICS ; SURFACE TREATMENT OF FIBRES OR FILAMENTS MADE FROM GLASS,MINERALS OR SLAGS ; SURFACE TREATMENT OF GLASS</subject><creationdate>2022</creationdate><oa>free_for_read</oa><woscitedreferencessubscribed>false</woscitedreferencessubscribed></display><links><openurl>$$Topenurl_article</openurl><openurlfulltext>$$Topenurlfull_article</openurlfulltext><thumbnail>$$Tsyndetics_thumb_exl</thumbnail><linktohtml>$$Uhttps://worldwide.espacenet.com/publicationDetails/biblio?FT=D&amp;date=20220811&amp;DB=EPODOC&amp;CC=WO&amp;NR=2022169902A1$$EHTML$$P50$$Gepo$$Hfree_for_read</linktohtml><link.rule.ids>230,308,780,885,25564,76547</link.rule.ids><linktorsrc>$$Uhttps://worldwide.espacenet.com/publicationDetails/biblio?FT=D&amp;date=20220811&amp;DB=EPODOC&amp;CC=WO&amp;NR=2022169902A1$$EView_record_in_European_Patent_Office$$FView_record_in_$$GEuropean_Patent_Office$$Hfree_for_read</linktorsrc></links><search><creatorcontrib>DYER, Robert</creatorcontrib><creatorcontrib>SAVRAN, Brian</creatorcontrib><creatorcontrib>STOLOV, Andrei</creatorcontrib><creatorcontrib>WESTBROOK, Paul</creatorcontrib><creatorcontrib>SOUNDARA, Vixay</creatorcontrib><creatorcontrib>HOKANSSON, Adam</creatorcontrib><creatorcontrib>POPELKA, Matthew</creatorcontrib><title>THERMALLY ANNEALED GRATINGS IN COATED FIBER AND RELATED SYSTEMS AND METHODS</title><description>Described herein are systems, methods, and articles of manufacture for a coated fiber modified by actinic radiation to increase back-scattering, which experiences very little back scattering decay at a temperature and time of exposure that is sufficient to noticeably degrade the coating and/or noticeably degrade the optical fiber due to outgassing of hydrogen from the coating, wherein an optical fiber comprises a fiber length, a coating having a treated coating weight, wherein the treated coating weight is at least 25% less of an original coating weight prior to an annealing treatment, and an optical back-scatter along the fiber length greater than a Rayleigh back-scattering over the fiber length, wherein the optical back-scatter does not decrease along the fiber length by more than 3 dB after exposure to annealing treatment. L'invention concerne des systèmes, des procédés, et des articles de fabrication pour une fibre revêtue modifiée par un rayonnement actinique pour augmenter la rétrodiffusion, qui subit une très faible décroissance de la rétrodiffusion à une température et un temps d'exposition qui est suffisant pour dégrader sensiblement le revêtement et/ou dégrader sensiblement la fibre optique due au dégazage de l'hydrogène du revêtement, une fibre optique comprenant une longueur de fibre, un revêtement ayant un poids de revêtement traité, le poids de revêtement traité étant d'au moins 25 % inférieur à un poids de revêtement d'origine avant un traitement de recuit, et une rétrodiffusion optique le long de la longueur de fibre supérieure à une rétrodiffusion de Rayleigh sur la longueur de la fibre, la rétrodiffusion optique ne diminuant pas le long de la longueur de fibre de plus de 3 dB après exposition à un traitement de recuit.</description><subject>CHEMICAL COMPOSITION OF GLASSES, GLAZES, OR VITREOUSENAMELS</subject><subject>CHEMISTRY</subject><subject>GLASS</subject><subject>JOINING GLASS TO GLASS OR OTHER MATERIALS</subject><subject>MANUFACTURE, SHAPING, OR SUPPLEMENTARY PROCESSES</subject><subject>METALLURGY</subject><subject>MINERAL OR SLAG WOOL</subject><subject>OPTICAL ELEMENTS, SYSTEMS, OR APPARATUS</subject><subject>OPTICS</subject><subject>PHYSICS</subject><subject>SURFACE TREATMENT OF FIBRES OR FILAMENTS MADE FROM GLASS,MINERALS OR SLAGS</subject><subject>SURFACE TREATMENT OF GLASS</subject><fulltext>true</fulltext><rsrctype>patent</rsrctype><creationdate>2022</creationdate><recordtype>patent</recordtype><sourceid>EVB</sourceid><recordid>eNrjZPAO8XAN8nX08YlUcPTzc3X0cXVRcA9yDPH0cw9W8PRTcPZ3DAEKuXk6uQYBVbgoBLn6gEWCI4NDXH2DwWK-riEe_i7BPAysaYk5xam8UJqbQdnNNcTZQze1ID8-tbggMTk1L7UkPtzfyMDIyNDM0tLAyNHQmDhVAB-xLk8</recordid><startdate>20220811</startdate><enddate>20220811</enddate><creator>DYER, Robert</creator><creator>SAVRAN, Brian</creator><creator>STOLOV, Andrei</creator><creator>WESTBROOK, Paul</creator><creator>SOUNDARA, Vixay</creator><creator>HOKANSSON, Adam</creator><creator>POPELKA, Matthew</creator><scope>EVB</scope></search><sort><creationdate>20220811</creationdate><title>THERMALLY ANNEALED GRATINGS IN COATED FIBER AND RELATED SYSTEMS AND METHODS</title><author>DYER, Robert ; SAVRAN, Brian ; STOLOV, Andrei ; WESTBROOK, Paul ; SOUNDARA, Vixay ; HOKANSSON, Adam ; POPELKA, Matthew</author></sort><facets><frbrtype>5</frbrtype><frbrgroupid>cdi_FETCH-epo_espacenet_WO2022169902A13</frbrgroupid><rsrctype>patents</rsrctype><prefilter>patents</prefilter><language>eng ; fre</language><creationdate>2022</creationdate><topic>CHEMICAL COMPOSITION OF GLASSES, GLAZES, OR VITREOUSENAMELS</topic><topic>CHEMISTRY</topic><topic>GLASS</topic><topic>JOINING GLASS TO GLASS OR OTHER MATERIALS</topic><topic>MANUFACTURE, SHAPING, OR SUPPLEMENTARY PROCESSES</topic><topic>METALLURGY</topic><topic>MINERAL OR SLAG WOOL</topic><topic>OPTICAL ELEMENTS, SYSTEMS, OR APPARATUS</topic><topic>OPTICS</topic><topic>PHYSICS</topic><topic>SURFACE TREATMENT OF FIBRES OR FILAMENTS MADE FROM GLASS,MINERALS OR SLAGS</topic><topic>SURFACE TREATMENT OF GLASS</topic><toplevel>online_resources</toplevel><creatorcontrib>DYER, Robert</creatorcontrib><creatorcontrib>SAVRAN, Brian</creatorcontrib><creatorcontrib>STOLOV, Andrei</creatorcontrib><creatorcontrib>WESTBROOK, Paul</creatorcontrib><creatorcontrib>SOUNDARA, Vixay</creatorcontrib><creatorcontrib>HOKANSSON, Adam</creatorcontrib><creatorcontrib>POPELKA, Matthew</creatorcontrib><collection>esp@cenet</collection></facets><delivery><delcategory>Remote Search Resource</delcategory><fulltext>fulltext_linktorsrc</fulltext></delivery><addata><au>DYER, Robert</au><au>SAVRAN, Brian</au><au>STOLOV, Andrei</au><au>WESTBROOK, Paul</au><au>SOUNDARA, Vixay</au><au>HOKANSSON, Adam</au><au>POPELKA, Matthew</au><format>patent</format><genre>patent</genre><ristype>GEN</ristype><title>THERMALLY ANNEALED GRATINGS IN COATED FIBER AND RELATED SYSTEMS AND METHODS</title><date>2022-08-11</date><risdate>2022</risdate><abstract>Described herein are systems, methods, and articles of manufacture for a coated fiber modified by actinic radiation to increase back-scattering, which experiences very little back scattering decay at a temperature and time of exposure that is sufficient to noticeably degrade the coating and/or noticeably degrade the optical fiber due to outgassing of hydrogen from the coating, wherein an optical fiber comprises a fiber length, a coating having a treated coating weight, wherein the treated coating weight is at least 25% less of an original coating weight prior to an annealing treatment, and an optical back-scatter along the fiber length greater than a Rayleigh back-scattering over the fiber length, wherein the optical back-scatter does not decrease along the fiber length by more than 3 dB after exposure to annealing treatment. L'invention concerne des systèmes, des procédés, et des articles de fabrication pour une fibre revêtue modifiée par un rayonnement actinique pour augmenter la rétrodiffusion, qui subit une très faible décroissance de la rétrodiffusion à une température et un temps d'exposition qui est suffisant pour dégrader sensiblement le revêtement et/ou dégrader sensiblement la fibre optique due au dégazage de l'hydrogène du revêtement, une fibre optique comprenant une longueur de fibre, un revêtement ayant un poids de revêtement traité, le poids de revêtement traité étant d'au moins 25 % inférieur à un poids de revêtement d'origine avant un traitement de recuit, et une rétrodiffusion optique le long de la longueur de fibre supérieure à une rétrodiffusion de Rayleigh sur la longueur de la fibre, la rétrodiffusion optique ne diminuant pas le long de la longueur de fibre de plus de 3 dB après exposition à un traitement de recuit.</abstract><oa>free_for_read</oa></addata></record>
fulltext fulltext_linktorsrc
identifier
ispartof
issn
language eng ; fre
recordid cdi_epo_espacenet_WO2022169902A1
source esp@cenet
subjects CHEMICAL COMPOSITION OF GLASSES, GLAZES, OR VITREOUSENAMELS
CHEMISTRY
GLASS
JOINING GLASS TO GLASS OR OTHER MATERIALS
MANUFACTURE, SHAPING, OR SUPPLEMENTARY PROCESSES
METALLURGY
MINERAL OR SLAG WOOL
OPTICAL ELEMENTS, SYSTEMS, OR APPARATUS
OPTICS
PHYSICS
SURFACE TREATMENT OF FIBRES OR FILAMENTS MADE FROM GLASS,MINERALS OR SLAGS
SURFACE TREATMENT OF GLASS
title THERMALLY ANNEALED GRATINGS IN COATED FIBER AND RELATED SYSTEMS AND METHODS
url https://sfx.bib-bvb.de/sfx_tum?ctx_ver=Z39.88-2004&ctx_enc=info:ofi/enc:UTF-8&ctx_tim=2024-12-29T10%3A42%3A23IST&url_ver=Z39.88-2004&url_ctx_fmt=infofi/fmt:kev:mtx:ctx&rfr_id=info:sid/primo.exlibrisgroup.com:primo3-Article-epo_EVB&rft_val_fmt=info:ofi/fmt:kev:mtx:patent&rft.genre=patent&rft.au=DYER,%20Robert&rft.date=2022-08-11&rft_id=info:doi/&rft_dat=%3Cepo_EVB%3EWO2022169902A1%3C/epo_EVB%3E%3Curl%3E%3C/url%3E&disable_directlink=true&sfx.directlink=off&sfx.report_link=0&rft_id=info:oai/&rft_id=info:pmid/&rfr_iscdi=true