SILVER/TITANIUM DIOXIDE IN-SITU LOADED BIOMASS MATERIAL BASED ON POLYDOPAMINE MODIFICATION AND PREPARATION METHOD THEREFOR

A silver/titanium dioxide in-situ loaded biomass material based on polydopamine modification and a preparation method therefor. The method comprises the following steps: impregnating a pretreated biomass material in a dopamine solution, adjusting a pH value to be 8-10 and performing stirring reactio...

Ausführliche Beschreibung

Gespeichert in:
Bibliographische Detailangaben
Hauptverfasser: XUE, Zhicheng, LIU, Yuan, HU, Jinbo, CHANG, Shanshan, ZHANG, Xiang, LU, Zhou, SHANG, Jianxiong, LIU, Gonggang, WU, Zhiping, ZHU, Xiu, LI, Xianjun
Format: Patent
Sprache:chi ; eng ; fre
Schlagworte:
Online-Zugang:Volltext bestellen
Tags: Tag hinzufügen
Keine Tags, Fügen Sie den ersten Tag hinzu!
Beschreibung
Zusammenfassung:A silver/titanium dioxide in-situ loaded biomass material based on polydopamine modification and a preparation method therefor. The method comprises the following steps: impregnating a pretreated biomass material in a dopamine solution, adjusting a pH value to be 8-10 and performing stirring reaction to obtain a polydopamine modified biomass material; first impregnating the polydopamine modified biomass material in a titanyl sulfate solution and then performing hydrolysis reaction in an alkaline solution having the pH value of 7-10 to obtain a titanium dioxide in-situ loaded biomass material; impregnating the obtained titanium dioxide in-situ loaded biomass material in a silver nitrate solution, performing reduction reaction, and drying the material to obtain the silver/titanium dioxide in-situ loaded biomass material. The method has the advantages that the method is simple, industrialization is easily implemented, a mildew-proof effect is good, and the like. L'invention concerne un matériau de biomasse charg