HAIRSPRING AND SPEED REGULATOR
This hairspring comprises SiO2 and Al2O3 in amounts of 60-70 mass% and 10-15 mass%, respectively, and comprises glass that substantially does not comprise an alkali metal oxide. Furthermore, the glass preferably comprises CaO in an amount of 5 mass% or more. Furthermore, the glass preferably substan...
Gespeichert in:
Hauptverfasser: | , |
---|---|
Format: | Patent |
Sprache: | eng ; fre ; jpn |
Schlagworte: | |
Online-Zugang: | Volltext bestellen |
Tags: |
Tag hinzufügen
Keine Tags, Fügen Sie den ersten Tag hinzu!
|
Zusammenfassung: | This hairspring comprises SiO2 and Al2O3 in amounts of 60-70 mass% and 10-15 mass%, respectively, and comprises glass that substantially does not comprise an alkali metal oxide. Furthermore, the glass preferably comprises CaO in an amount of 5 mass% or more. Furthermore, the glass preferably substantially does not comprise ZnO. The hairspring preferably has a coefficient of thermal expansion of no less than 3.0 × 10-6/K and less than 4.0 × 10-6/K.
Ce ressort spiral comprend SiO2 et Al2O3 dans des quantités de 60 à 70 % en masse et 10 à 15 % en masse, respectivement, et comprend du verre qui ne comprend sensiblement pas d'oxyde de métal alcalin. De plus, le verre comprend de préférence CaO en une quantité égale ou supérieure à 5 % en masse. Et le verre ne comprend sensiblement pas, de préférence, ZnO. Le ressort spiral présente de préférence un coefficient de dilatation thermique non inférieur à 3,0 × 10-6/K et inférieur à 4,0 × 10-6/K.
ひげぜんまいは、SiO2を60~70質量%、Al2O3を10~15質量%の量で含み、実質的にアルカリ金属酸化物を含まないガラスを含む。上記ガラスは、さらにCaOを5質量%以上の量で含むことが好ましい。上記ガラスは、さらに、実質的にZnOを含まないことが好ましい。上記ひげぜんまいは、熱膨張率が、3.0×10-6/K以上4.0×10-6/K未満であることが好ましい。 |
---|