METHOD FOR MAKING SOOT PREFORMS AND GLASS OPTICAL FIBERS

A method of forming an optical fiber includes the steps of forming a soot blank of a silica-based cladding material, wherein the soot blank has a top surface and a bulk density of between 0.8 g/cm2 and 1.6 g/cm3. At least one hole is drilled in the top surface of the soot blank. At least one core ca...

Ausführliche Beschreibung

Gespeichert in:
Bibliographische Detailangaben
Hauptverfasser: LUO, XIAOMING, MCCARTHY, JOSEPH EDWARD, LI, MING-JUN, TANDON, PUSHKAR, ZHOU, CHUNFENG, PENG, GAOZHU, STONE, JEFFERY SCOTT
Format: Patent
Sprache:eng ; fre
Schlagworte:
Online-Zugang:Volltext bestellen
Tags: Tag hinzufügen
Keine Tags, Fügen Sie den ersten Tag hinzu!
Beschreibung
Zusammenfassung:A method of forming an optical fiber includes the steps of forming a soot blank of a silica-based cladding material, wherein the soot blank has a top surface and a bulk density of between 0.8 g/cm2 and 1.6 g/cm3. At least one hole is drilled in the top surface of the soot blank. At least one core cane member is positioned in the at least one hole. The soot blank and at least one soot core cane member are consolidated to form a consolidated preform. The consolidated preform is drawn into an optical fiber. La présente invention concerne un procédé de formation d'une fibre optique comprenant les étapes consistant à former une ébauche de suie d'un matériau de gainage à base de silice, l'ébauche de suie ayant une surface supérieure et une masse volumique comprise entre 0,8 g/cm3 et 1,6 g/cm3. Au moins un trou est percé dans la surface supérieure de l'ébauche de suie. Au moins un élément tige centrale est positionné dans ledit trou. L'ébauche de suie et au moins un élément tige centrale de suie sont consolidés de manière à former une préforme consolidée. La préforme consolidée est étirée en une fibre optique.