HONEYCOMB PAPER
A consolidated fibrous mat comprises 20 to 50 weight percent of reinforcing fibers; and a continuous phase connecting the reinforcing fibers, comprising 50 to 70 weight percent of a polymer having a melt temperature at least 20°C lower than the reinforcing fibers, and 5 to 10 weight percent of a bin...
Gespeichert in:
Hauptverfasser: | , , , , , , |
---|---|
Format: | Patent |
Sprache: | eng ; fre |
Schlagworte: | |
Online-Zugang: | Volltext bestellen |
Tags: |
Tag hinzufügen
Keine Tags, Fügen Sie den ersten Tag hinzu!
|
Zusammenfassung: | A consolidated fibrous mat comprises 20 to 50 weight percent of reinforcing fibers; and a continuous phase connecting the reinforcing fibers, comprising 50 to 70 weight percent of a polymer having a melt temperature at least 20°C lower than the reinforcing fibers, and 5 to 10 weight percent of a binder having a melt temperature lower than the polymer; wherein the weight percent of each of the reinforcing fibers, the polymer, and the binder is based on the combined total weight of the reinforcing fibers, the polymer, and the binder.
L'invention concerne une natte fibreuse tassée comportant 20 à 50 pour cent en poids de fibres de renfort ; et une phase continue liant les fibres de renfort, comportant 50 à 70 pour cent en poids d'un polymère présentant une température de fusion inférieure d'au moins 20°C à celle des fibres de renfort, ainsi que 5 à 10 pour cent en poids d'un liant présentant une température de fusion inférieure à celle du polymère ; le pourcentage en poids de chaque composant parmi les fibres de renfort, le polymère et le liant étant basé sur le poids total combiné des fibres de renfort, du polymère et du liant. |
---|