METHOD FOR TREATING STEEL FOR DIRECTIONAL ELECTROMAGNETIC STEEL PLATE AND METHOD FOR PRODUCING DIRECTIONAL ELECTROMAGNETIC STEEL PLATE
The surface temperature of a slab is reduced so as not to exceed 600°C from the start of the continuous casting (step S2) to the start of the slab reheating (step S3). The surface temperature of the slab is maintained at a temperature of at least 150°C from the start of continuous casting (step S2)...
Gespeichert in:
Hauptverfasser: | , , , |
---|---|
Format: | Patent |
Sprache: | eng ; fre ; jpn |
Schlagworte: | |
Online-Zugang: | Volltext bestellen |
Tags: |
Tag hinzufügen
Keine Tags, Fügen Sie den ersten Tag hinzu!
|
Zusammenfassung: | The surface temperature of a slab is reduced so as not to exceed 600°C from the start of the continuous casting (step S2) to the start of the slab reheating (step S3). The surface temperature of the slab is maintained at a temperature of at least 150°C from the start of continuous casting (step S2) to the start of slab reheating (S3). The surface temperature of the slab during slab reheating (step S3) is maintained between 1080°C and 1200°C.
La température de surface d'une brame est réduite de façon à ne pas dépasser 600 °C entre le début de la coulée continue (étape S2) et le début du réchauffage de la brame (étape S3). La température de surface de la brame est maintenue à une température d'au moins 150 °C entre le début de la coulée continue (étape S2) et le début du réchauffage de la brame (S3). La température de surface de la brame pendant le réchauffage de la brame (étape S3) est maintenue entre 1080 °C et 1200 °C. |
---|