METHODS AND APPARATUS FOR REDUCING PLATINUM-GROUP DEFECTS IN SHEET GLASS
A substantially-isolated/controlled, limited-volume, gas-filled space (e.g., 113b) is formed over at least one free (open) surface of flowing molten glass in a manufacturing line used to produce glass sheets (137), e.g., a manufacturing line employing the fusion process to produce glass sheets suita...