Ingot for bearing and production process

A method is provided with which a bearing steel, even when obtained from an ingot, is made to have a segregation part reduced in the degree of segregation and maximum inclusion diameter. The ingot contains 0.56-0.70 mass % C, 0.15-0.50 mass %, excluding 0.50 mass %, Si, 0.60-1.50 mass % Mn, 0.50-1.1...

Ausführliche Beschreibung

Gespeichert in:
Bibliographische Detailangaben
Hauptverfasser: Uwai Kiyoshi, Mitao Shinji, Honjo Minoru
Format: Patent
Sprache:eng
Schlagworte:
Online-Zugang:Volltext bestellen
Tags: Tag hinzufügen
Keine Tags, Fügen Sie den ersten Tag hinzu!
Beschreibung
Zusammenfassung:A method is provided with which a bearing steel, even when obtained from an ingot, is made to have a segregation part reduced in the degree of segregation and maximum inclusion diameter. The ingot contains 0.56-0.70 mass % C, 0.15-0.50 mass %, excluding 0.50 mass %, Si, 0.60-1.50 mass % Mn, 0.50-1.10 mass % Cr, 0.05-0.5 mass % Mo, up to 0.025 mass % P, up to 0.025 mass % S, 0.005-0.500 mass % Al, up to 0.0015 mass % O, and 0.0030-0.015 mass % N, with the remainder comprising Fe and incidental impurities. The ingot has a degree of segregation of 2.8 or less and a predicted value of the maximum diameter of inclusions present in 30,000 mm2 of the ingot, as calculated by extreme value statistics, of 60 μm or less.