Multilayered articles with low optical retardation

A coextruded multilayered thermoplastic article including: a first layer with a first surface texture, wherein the first layer comprises a first transparent thermoplastic polymer having a first stress optical coefficient (Cm1) measured at 20° C. above the glass transition temperature of the first po...

Ausführliche Beschreibung

Gespeichert in:
Bibliographische Detailangaben
Hauptverfasser: Zhou Yuan, Bastawros Adel, Feng Wei, Wang Zhi, Zhou Jian
Format: Patent
Sprache:eng
Schlagworte:
Online-Zugang:Volltext bestellen
Tags: Tag hinzufügen
Keine Tags, Fügen Sie den ersten Tag hinzu!
Beschreibung
Zusammenfassung:A coextruded multilayered thermoplastic article including: a first layer with a first surface texture, wherein the first layer comprises a first transparent thermoplastic polymer having a first stress optical coefficient (Cm1) measured at 20° C. above the glass transition temperature of the first polymer; a second layer located comprising a second transparent thermoplastic polymer having a second stress optical coefficient (Cm2) measured at 20° C. above the glass transition temperature of the second matrix; wherein a relation between the first stress optical coefficient and the second stress optical coefficient is Cm2>4(Cm1) (Formula A) wherein the thickness of the first layer measured from the highest peaks of the first surface texture to the second side of the first layer is greater than 1.5 times Rz of the first surface texture but less than or equal to 75% of the total thickness of the article.