Silicon oxide, making method, negative electrode, lithium ion secondary battery, and electrochemical capacitor
Particulate silicon oxide having a Cu content of 100-20,000 ppm, an Fe content of 20-1,000 ppm, an Al content of up to 1,000 ppm, an average particle size of 0.1-30 μm, and a BET specific surface area of 0.5-30 m2/g is used as negative electrode material in constructing a nonaqueous electrolyte seco...
Gespeichert in:
Hauptverfasser: | , , , |
---|---|
Format: | Patent |
Sprache: | eng |
Schlagworte: | |
Online-Zugang: | Volltext bestellen |
Tags: |
Tag hinzufügen
Keine Tags, Fügen Sie den ersten Tag hinzu!
|
Zusammenfassung: | Particulate silicon oxide having a Cu content of 100-20,000 ppm, an Fe content of 20-1,000 ppm, an Al content of up to 1,000 ppm, an average particle size of 0.1-30 μm, and a BET specific surface area of 0.5-30 m2/g is used as negative electrode material in constructing a nonaqueous electrolyte secondary battery. The secondary battery is improved in cycle performance while maintaining the high battery capacity and low volume expansion of silicon oxide. |
---|