Process for the production of grain-oriented magnetic sheet starting from thin slab
A process for producing grain oriented magnetic sheets by subjecting a steel slab 100 mm, containing 2.5-3.5% si, to the following operations: optional first heating, to a temperature T1 1250° C.; first rough hot-rolling at T2 between 900 and 1200° C., the reduction ratio (% Rid) being at least 80%...
Gespeichert in:
Hauptverfasser: | , , |
---|---|
Format: | Patent |
Sprache: | eng |
Schlagworte: | |
Online-Zugang: | Volltext bestellen |
Tags: |
Tag hinzufügen
Keine Tags, Fügen Sie den ersten Tag hinzu!
|
Zusammenfassung: | A process for producing grain oriented magnetic sheets by subjecting a steel slab 100 mm, containing 2.5-3.5% si, to the following operations: optional first heating, to a temperature T1 1250° C.; first rough hot-rolling at T2 between 900 and 1200° C., the reduction ratio (% Rid) being at least 80% in the absence of a subsequent heating or, in the presence of a subsequent heating to T3 1300° C., at least 60% determined by % Rid=80−(T3−T2)/5; second finishing hot-rolling at T4 |
---|