Production method of aromatic polycarbonate

The object of the present invention is to provide a production method for an aromatic polycarbonate, in which eye boogers at the time of extrusion molding are reduced, and a continuous operation for a long period of time is possible. The present invention relates to a method when an extrusion moldin...

Ausführliche Beschreibung

Gespeichert in:
Bibliographische Detailangaben
Hauptverfasser: MURAKAMI HIDEKI, UCHIMURA RYUUJI
Format: Patent
Sprache:eng
Schlagworte:
Online-Zugang:Volltext bestellen
Tags: Tag hinzufügen
Keine Tags, Fügen Sie den ersten Tag hinzu!
Beschreibung
Zusammenfassung:The object of the present invention is to provide a production method for an aromatic polycarbonate, in which eye boogers at the time of extrusion molding are reduced, and a continuous operation for a long period of time is possible. The present invention relates to a method when an extrusion molding is produced using an extruder in which a tapered part 1 has a half apex angle of from 4 to 20° formed at the outlet part of a die hole 9, and outlet parts of plural die holes 9 are arranged in a staggered state at the resin discharge surface side of a die plate 10, the shear rate γ at the extruder outlet is from 100 to 500 sec−1, and the shear stress τ is from 50 to 200 kPa.