Double anneal with improved reliability for dual contact etch stop liner scheme

A method for forming a device with both PFET and NFET transistors using a PFET compressive etch stop liner and a NFET tensile etch stop liner and two anneals in a deuterium containing atmosphere. The method comprises: providing a NFET transistor in a NFET region and a PFET transistor in a PFET regio...

Ausführliche Beschreibung

Gespeichert in:
Bibliographische Detailangaben
Hauptverfasser: FEN JAMIN F, LIM ENG HUA, LIN WENHE, LIM KHEE YONG, CHAN VICTOR
Format: Patent
Sprache:eng
Schlagworte:
Online-Zugang:Volltext bestellen
Tags: Tag hinzufügen
Keine Tags, Fügen Sie den ersten Tag hinzu!
Beschreibung
Zusammenfassung:A method for forming a device with both PFET and NFET transistors using a PFET compressive etch stop liner and a NFET tensile etch stop liner and two anneals in a deuterium containing atmosphere. The method comprises: providing a NFET transistor in a NFET region and a PFET transistor in a PFET region. We form a NFET tensile contact etch-stop liner over the NFET region. Then we perform a first deuterium anneal. We form a PFET compressive etch stop liner over the PFET region. We form a (ILD) dielectric layer with contact openings over the substrate. We perform a second deuterium anneal. The temperature of the second deuterium anneal is less than the temperature of the first deuterium anneal.