Chromium removal from leach liquors produced during high pressure acid leaching of lateritic ores
A method is provided for the removal of chromium from leach liquors produced during high pressure leaching of laterite ores in an autoclave, by addition to the autoclave of carbon in a quantity of about 0.5%-1% by weight with reference to the total dry feed.
Gespeichert in:
Hauptverfasser: | , , , , |
---|---|
Format: | Patent |
Sprache: | eng |
Schlagworte: | |
Online-Zugang: | Volltext bestellen |
Tags: |
Tag hinzufügen
Keine Tags, Fügen Sie den ersten Tag hinzu!
|
Zusammenfassung: | A method is provided for the removal of chromium from leach liquors produced during high pressure leaching of laterite ores in an autoclave, by addition to the autoclave of carbon in a quantity of about 0.5%-1% by weight with reference to the total dry feed. |
---|