Solvent-resistant textile binder

PCT No. PCT/EP95/03623 Sec. 371 Date Mar. 12, 1997 Sec. 102(e) Date Mar. 12, 1997 PCT Filed Sep. 14, 1995 PCT Pub. No. WO96/08597 PCT Pub. Date Mar. 21, 1996The invention provides a process for improving the resistance to solvents in finishing and stabilizing fiber materials with textile binders, wh...

Ausführliche Beschreibung

Gespeichert in:
Bibliographische Detailangaben
Hauptverfasser: LUMPP, ANDREAS, KOEGLER, GERHARD
Format: Patent
Sprache:eng
Schlagworte:
Online-Zugang:Volltext bestellen
Tags: Tag hinzufügen
Keine Tags, Fügen Sie den ersten Tag hinzu!
Beschreibung
Zusammenfassung:PCT No. PCT/EP95/03623 Sec. 371 Date Mar. 12, 1997 Sec. 102(e) Date Mar. 12, 1997 PCT Filed Sep. 14, 1995 PCT Pub. No. WO96/08597 PCT Pub. Date Mar. 21, 1996The invention provides a process for improving the resistance to solvents in finishing and stabilizing fiber materials with textile binders, wherein the textile binder used is an aqueous copolymer dispersion or a redispersible copolymer powder of copolymers with a Tg of -60 DEG C. to +60 DEG C., containing (a) one or more monomer units from the group consisting of vinyl esters of unbranched or branched carboxyli acids with 1 to 12 carbon atoms, esters of acrylic acid and methacrylic acid with unbranched or branched alcohols with 1 to 12 carbon atoms, vinyl aromatics, vinyl halides and alpha -olefins, and (b) 0.3 to 10 wt %, relative to the total weight of the copolymer, of one or more N-(alkoxymethyl)-acrylamides or N-(alkoxymethyl)methacrylamides with a C1-C6 alkyl residue, or mixtures of these N-(alkoxymethyl)-meth(acrylamides with N-Methylolacrylamide and/or N-methylolmethacrylamide in a weight ratio of N-methylol compound to N-(alkoxymethyl) compound of at most 5:1.