Preparation of polyisobutylsuccinic anhydrides

Polyisobutylsuccinic anhydrides having an average molar ratio of succinic anhydride groups to polyisobutyl groups of from 1.05:1 to 1.3:1 are prepared by reacting polyisobutene having an average molecular weight Mw of 600-5000 and containing at least 70% of terminal double bonds with maleic anhydrid...

Ausführliche Beschreibung

Gespeichert in:
Bibliographische Detailangaben
Hauptverfasser: OPPENLAENDER, KNUT, GREIF, NORBERT
Format: Patent
Sprache:eng
Schlagworte:
Online-Zugang:Volltext bestellen
Tags: Tag hinzufügen
Keine Tags, Fügen Sie den ersten Tag hinzu!
Beschreibung
Zusammenfassung:Polyisobutylsuccinic anhydrides having an average molar ratio of succinic anhydride groups to polyisobutyl groups of from 1.05:1 to 1.3:1 are prepared by reacting polyisobutene having an average molecular weight Mw of 600-5000 and containing at least 70% of terminal double bonds with maleic anhydride in a molar ratio of maleic anhydride to polyisobutene of from 1.05:1 to 3:1 at 160 DEG -210 DEG C. in the presence of a catalytic amount of a dicarboxylic acid of 2 to 6 carbon atoms.