Silicon steel sheets having low iron loss and method of producing the same
A silicon-containing steel sheet having a low iron loss has such a crystal structure that crystal grains having an inclination angle of {110} face of not more than 10 DEG with respect to the sheet surface are included in an amount of not less than 80 vol % and exhibit a graining surface pattern in w...
Gespeichert in:
Hauptverfasser: | , , , , , , , , , |
---|---|
Format: | Patent |
Sprache: | eng |
Schlagworte: | |
Online-Zugang: | Volltext bestellen |
Tags: |
Tag hinzufügen
Keine Tags, Fügen Sie den ersten Tag hinzu!
|
Zusammenfassung: | A silicon-containing steel sheet having a low iron loss has such a crystal structure that crystal grains having an inclination angle of {110} face of not more than 10 DEG with respect to the sheet surface are included in an amount of not less than 80 vol % and exhibit a graining surface pattern in which boundaries of these crystal grains form stepwise difference or groove of not less than 0.4 mu m as a maximum height. This sheet is produced by subjecting a grain oriented silicon steel sheet after final annealing to a magnetically smoothening treatment by electrolysis in an squeous solution containing at least one of water soluble halides. |
---|