Composite rubber material and process for making same
An improved composite rubber material having a baked layer of fluorine resin of 10 microns to about 1 millimeter in thickness is proposed. The coated layer of fluorine resin is baked at a temperature over 400 DEG C. for not more than 7 minutes. This assures that the fluorine resin is baked without d...
Gespeichert in:
Hauptverfasser: | , , , |
---|---|
Format: | Patent |
Sprache: | eng |
Schlagworte: | |
Online-Zugang: | Volltext bestellen |
Tags: |
Tag hinzufügen
Keine Tags, Fügen Sie den ersten Tag hinzu!
|
Zusammenfassung: | An improved composite rubber material having a baked layer of fluorine resin of 10 microns to about 1 millimeter in thickness is proposed. The coated layer of fluorine resin is baked at a temperature over 400 DEG C. for not more than 7 minutes. This assures that the fluorine resin is baked without deteriorating the rubber material. |
---|