Method for producing a precursor pitch for carbon fiber

A precursor pitch suitable for production of carbon fiber which is excellent in thermal stability, spinnability, infusibility and is few in impurities, is produced by heating a coal tar pitch at a temperature of 350 DEG -500 DEG C. to form mesophase and extracting the thus heated pitch with a tar se...

Ausführliche Beschreibung

Gespeichert in:
Bibliographische Detailangaben
Hauptverfasser: YUDATE, KOZO, NAGASAWA, KEN
Format: Patent
Sprache:eng
Schlagworte:
Online-Zugang:Volltext bestellen
Tags: Tag hinzufügen
Keine Tags, Fügen Sie den ersten Tag hinzu!
Beschreibung
Zusammenfassung:A precursor pitch suitable for production of carbon fiber which is excellent in thermal stability, spinnability, infusibility and is few in impurities, is produced by heating a coal tar pitch at a temperature of 350 DEG -500 DEG C. to form mesophase and extracting the thus heated pitch with a tar series light oil to obtain the precursor pitch.