Method and electrolytic bath for the deposition of low carat bright gold-silver alloy coatings

Bright, low carat gold-silver-alloy coatings which are ductile and have a thickness up to over 100 mu m are obtained from an electrolytic bath containing 0.5 to 25 g/l of gold in the form of alkali gold cyanide, 0.25 to 15 g/l of silver in the form of alkali silver cyanide and 10 to 200 g/l of alkal...

Ausführliche Beschreibung

Gespeichert in:
Bibliographische Detailangaben
Hauptverfasser: GIESECKE, NORBERT, DORBATH, BERND, SCHLODDER, RAINER
Format: Patent
Sprache:eng
Schlagworte:
Online-Zugang:Volltext bestellen
Tags: Tag hinzufügen
Keine Tags, Fügen Sie den ersten Tag hinzu!
Beschreibung
Zusammenfassung:Bright, low carat gold-silver-alloy coatings which are ductile and have a thickness up to over 100 mu m are obtained from an electrolytic bath containing 0.5 to 25 g/l of gold in the form of alkali gold cyanide, 0.25 to 15 g/l of silver in the form of alkali silver cyanide and 10 to 200 g/l of alkali cyanide as well as 0.001 to 5 g/l of tellurium in the form of a water soluble tellurium compound.