Method of preparing silicon from sodium fluosilicate

A process for preparing high purity silicon metal from Na2SiF6 (sodium fluosilicate). The sodium fluosilicate is heated to decomposition temperature to form NaF, which retains most of the impurities, and gaseous SiF4. The SiF4 is then reduced by the bomb reduction method using a reductant having a l...

Ausführliche Beschreibung

Gespeichert in:
Bibliographische Detailangaben
Hauptverfasser: SCHMIDT, FREDERICK A, REHBEIN, DAVID, CHIOTTI, PREMO
Format: Patent
Sprache:eng
Schlagworte:
Online-Zugang:Volltext bestellen
Tags: Tag hinzufügen
Keine Tags, Fügen Sie den ersten Tag hinzu!
Beschreibung
Zusammenfassung:A process for preparing high purity silicon metal from Na2SiF6 (sodium fluosilicate). The sodium fluosilicate is heated to decomposition temperature to form NaF, which retains most of the impurities, and gaseous SiF4. The SiF4 is then reduced by the bomb reduction method using a reductant having a low packing density.