Washed wood pulp from a continuous digester is treated with oxygen in the blow line from the digester. Most of the treatment occurs within the mixer. The mixer has a mixing zone with a swept area of 10,000 to 1,000,000 square meters per metric ton of oven-dry pulp. A preferred range is 25,000 to 150...

Ausführliche Beschreibung

Gespeichert in:
Bibliographische Detailangaben
Hauptverfasser: BEPPLE, HENRY, BENTVELZEN, JOZEF M, TORREGROSSA, LOUIS O, BATTAN, HOWARD R, MEREDITH, MICHAEL D, JUSTICE, DENNIS H
Format: Patent
Sprache:eng
Schlagworte:
Online-Zugang:Volltext bestellen
Tags: Tag hinzufügen
Keine Tags, Fügen Sie den ersten Tag hinzu!
Beschreibung
Zusammenfassung:Washed wood pulp from a continuous digester is treated with oxygen in the blow line from the digester. Most of the treatment occurs within the mixer. The mixer has a mixing zone with a swept area of 10,000 to 1,000,000 square meters per metric ton of oven-dry pulp. A preferred range is 25,000 to 150,000 square meters per ton of oven-dry pulp and an optimum range is around 65,400 square meters per metric ton of oven-dry pulp. Following mixing, the pulp may be taken to a subsequent process, a diffusion washer, or to a storage tank.