Polyester stabilization process and product

A method for minimizing low temperature shrinkage of an axially-oriented polyester which includes heating the polyester out of contact with any surface by employing impinging heated gas at a temperature of about 140 DEG to about 180 DEG C. for a time between about 15 and about 3 seconds, and stabili...

Ausführliche Beschreibung

Gespeichert in:
Bibliographische Detailangaben
Hauptverfasser: PRICE, ROBERT L, BARTKUS, EDWARD A
Format: Patent
Sprache:eng
Schlagworte:
Online-Zugang:Volltext bestellen
Tags: Tag hinzufügen
Keine Tags, Fügen Sie den ersten Tag hinzu!
container_end_page
container_issue
container_start_page
container_title
container_volume
creator PRICE
ROBERT L
BARTKUS
EDWARD A
description A method for minimizing low temperature shrinkage of an axially-oriented polyester which includes heating the polyester out of contact with any surface by employing impinging heated gas at a temperature of about 140 DEG to about 180 DEG C. for a time between about 15 and about 3 seconds, and stabilized polyester obtained thereby.
format Patent
fullrecord <record><control><sourceid>epo_EVB</sourceid><recordid>TN_cdi_epo_espacenet_US4275107A</recordid><sourceformat>XML</sourceformat><sourcesystem>PC</sourcesystem><sourcerecordid>US4275107A</sourcerecordid><originalsourceid>FETCH-epo_espacenet_US4275107A3</originalsourceid><addsrcrecordid>eNrjZNAOyM-pTC0uSS1SKC5JTMrMyaxKLMnMz1MoKMpPTi0uVkjMSwGxU0qTS3gYWNMSc4pTeaE0N4O8m2uIs4duakF-fGpxQWJyal5qSXxosImRuamhgbmjMWEVAA_sKWc</addsrcrecordid><sourcetype>Open Access Repository</sourcetype><iscdi>true</iscdi><recordtype>patent</recordtype></control><display><type>patent</type><title>Polyester stabilization process and product</title><source>esp@cenet</source><creator>PRICE; ROBERT L ; BARTKUS; EDWARD A</creator><creatorcontrib>PRICE; ROBERT L ; BARTKUS; EDWARD A</creatorcontrib><description>A method for minimizing low temperature shrinkage of an axially-oriented polyester which includes heating the polyester out of contact with any surface by employing impinging heated gas at a temperature of about 140 DEG to about 180 DEG C. for a time between about 15 and about 3 seconds, and stabilized polyester obtained thereby.</description><language>eng</language><subject>AFTER-TREATMENT OF THE SHAPED PRODUCTS, e.g. REPAIRING ; PERFORMING OPERATIONS ; PRODUCING PARTICULAR ARTICLES FROM PLASTICS OR FROM SUBSTANCESIN A PLASTIC STATE ; SHAPING OF MATERIAL IN A PLASTIC STATE, NOT OTHERWISE PROVIDEDFOR ; SHAPING OR JOINING OF PLASTICS ; TRANSPORTING ; WORKING OF PLASTICS ; WORKING OF SUBSTANCES IN A PLASTIC STATE, IN GENERAL</subject><creationdate>1981</creationdate><oa>free_for_read</oa><woscitedreferencessubscribed>false</woscitedreferencessubscribed></display><links><openurl>$$Topenurl_article</openurl><openurlfulltext>$$Topenurlfull_article</openurlfulltext><thumbnail>$$Tsyndetics_thumb_exl</thumbnail><linktohtml>$$Uhttps://worldwide.espacenet.com/publicationDetails/biblio?FT=D&amp;date=19810623&amp;DB=EPODOC&amp;CC=US&amp;NR=4275107A$$EHTML$$P50$$Gepo$$Hfree_for_read</linktohtml><link.rule.ids>230,308,780,885,25564,76547</link.rule.ids><linktorsrc>$$Uhttps://worldwide.espacenet.com/publicationDetails/biblio?FT=D&amp;date=19810623&amp;DB=EPODOC&amp;CC=US&amp;NR=4275107A$$EView_record_in_European_Patent_Office$$FView_record_in_$$GEuropean_Patent_Office$$Hfree_for_read</linktorsrc></links><search><creatorcontrib>PRICE; ROBERT L</creatorcontrib><creatorcontrib>BARTKUS; EDWARD A</creatorcontrib><title>Polyester stabilization process and product</title><description>A method for minimizing low temperature shrinkage of an axially-oriented polyester which includes heating the polyester out of contact with any surface by employing impinging heated gas at a temperature of about 140 DEG to about 180 DEG C. for a time between about 15 and about 3 seconds, and stabilized polyester obtained thereby.</description><subject>AFTER-TREATMENT OF THE SHAPED PRODUCTS, e.g. REPAIRING</subject><subject>PERFORMING OPERATIONS</subject><subject>PRODUCING PARTICULAR ARTICLES FROM PLASTICS OR FROM SUBSTANCESIN A PLASTIC STATE</subject><subject>SHAPING OF MATERIAL IN A PLASTIC STATE, NOT OTHERWISE PROVIDEDFOR</subject><subject>SHAPING OR JOINING OF PLASTICS</subject><subject>TRANSPORTING</subject><subject>WORKING OF PLASTICS</subject><subject>WORKING OF SUBSTANCES IN A PLASTIC STATE, IN GENERAL</subject><fulltext>true</fulltext><rsrctype>patent</rsrctype><creationdate>1981</creationdate><recordtype>patent</recordtype><sourceid>EVB</sourceid><recordid>eNrjZNAOyM-pTC0uSS1SKC5JTMrMyaxKLMnMz1MoKMpPTi0uVkjMSwGxU0qTS3gYWNMSc4pTeaE0N4O8m2uIs4duakF-fGpxQWJyal5qSXxosImRuamhgbmjMWEVAA_sKWc</recordid><startdate>19810623</startdate><enddate>19810623</enddate><creator>PRICE; ROBERT L</creator><creator>BARTKUS; EDWARD A</creator><scope>EVB</scope></search><sort><creationdate>19810623</creationdate><title>Polyester stabilization process and product</title><author>PRICE; ROBERT L ; BARTKUS; EDWARD A</author></sort><facets><frbrtype>5</frbrtype><frbrgroupid>cdi_FETCH-epo_espacenet_US4275107A3</frbrgroupid><rsrctype>patents</rsrctype><prefilter>patents</prefilter><language>eng</language><creationdate>1981</creationdate><topic>AFTER-TREATMENT OF THE SHAPED PRODUCTS, e.g. REPAIRING</topic><topic>PERFORMING OPERATIONS</topic><topic>PRODUCING PARTICULAR ARTICLES FROM PLASTICS OR FROM SUBSTANCESIN A PLASTIC STATE</topic><topic>SHAPING OF MATERIAL IN A PLASTIC STATE, NOT OTHERWISE PROVIDEDFOR</topic><topic>SHAPING OR JOINING OF PLASTICS</topic><topic>TRANSPORTING</topic><topic>WORKING OF PLASTICS</topic><topic>WORKING OF SUBSTANCES IN A PLASTIC STATE, IN GENERAL</topic><toplevel>online_resources</toplevel><creatorcontrib>PRICE; ROBERT L</creatorcontrib><creatorcontrib>BARTKUS; EDWARD A</creatorcontrib><collection>esp@cenet</collection></facets><delivery><delcategory>Remote Search Resource</delcategory><fulltext>fulltext_linktorsrc</fulltext></delivery><addata><au>PRICE; ROBERT L</au><au>BARTKUS; EDWARD A</au><format>patent</format><genre>patent</genre><ristype>GEN</ristype><title>Polyester stabilization process and product</title><date>1981-06-23</date><risdate>1981</risdate><abstract>A method for minimizing low temperature shrinkage of an axially-oriented polyester which includes heating the polyester out of contact with any surface by employing impinging heated gas at a temperature of about 140 DEG to about 180 DEG C. for a time between about 15 and about 3 seconds, and stabilized polyester obtained thereby.</abstract><oa>free_for_read</oa></addata></record>
fulltext fulltext_linktorsrc
identifier
ispartof
issn
language eng
recordid cdi_epo_espacenet_US4275107A
source esp@cenet
subjects AFTER-TREATMENT OF THE SHAPED PRODUCTS, e.g. REPAIRING
PERFORMING OPERATIONS
PRODUCING PARTICULAR ARTICLES FROM PLASTICS OR FROM SUBSTANCESIN A PLASTIC STATE
SHAPING OF MATERIAL IN A PLASTIC STATE, NOT OTHERWISE PROVIDEDFOR
SHAPING OR JOINING OF PLASTICS
TRANSPORTING
WORKING OF PLASTICS
WORKING OF SUBSTANCES IN A PLASTIC STATE, IN GENERAL
title Polyester stabilization process and product
url https://sfx.bib-bvb.de/sfx_tum?ctx_ver=Z39.88-2004&ctx_enc=info:ofi/enc:UTF-8&ctx_tim=2025-01-06T00%3A29%3A22IST&url_ver=Z39.88-2004&url_ctx_fmt=infofi/fmt:kev:mtx:ctx&rfr_id=info:sid/primo.exlibrisgroup.com:primo3-Article-epo_EVB&rft_val_fmt=info:ofi/fmt:kev:mtx:patent&rft.genre=patent&rft.au=PRICE;%20ROBERT%20L&rft.date=1981-06-23&rft_id=info:doi/&rft_dat=%3Cepo_EVB%3EUS4275107A%3C/epo_EVB%3E%3Curl%3E%3C/url%3E&disable_directlink=true&sfx.directlink=off&sfx.report_link=0&rft_id=info:oai/&rft_id=info:pmid/&rfr_iscdi=true