Polyester stabilization process and product
A method for minimizing low temperature shrinkage of an axially-oriented polyester which includes heating the polyester out of contact with any surface by employing impinging heated gas at a temperature of about 140 DEG to about 180 DEG C. for a time between about 15 and about 3 seconds, and stabili...
Gespeichert in:
Hauptverfasser: | , , , |
---|---|
Format: | Patent |
Sprache: | eng |
Schlagworte: | |
Online-Zugang: | Volltext bestellen |
Tags: |
Tag hinzufügen
Keine Tags, Fügen Sie den ersten Tag hinzu!
|
Zusammenfassung: | A method for minimizing low temperature shrinkage of an axially-oriented polyester which includes heating the polyester out of contact with any surface by employing impinging heated gas at a temperature of about 140 DEG to about 180 DEG C. for a time between about 15 and about 3 seconds, and stabilized polyester obtained thereby. |
---|