Room temperature cured elastomer

Hydroxy terminated polybutadiene is reacted with naphtyl-potassium and 1-bromo-2,4-pentadiene in successive steps to form a bis(1,3-pentadienyl ether) derivative. Then the bismaleimide of dimer diamine is added to the polybutadiene derivative whereby a room temperature cure to an elastomer is achiev...

Ausführliche Beschreibung

Gespeichert in:
Bibliographische Detailangaben
Hauptverfasser: MARTIN, EUGENE C, ADICOFF, ARNOLD
Format: Patent
Sprache:eng
Schlagworte:
Online-Zugang:Volltext bestellen
Tags: Tag hinzufügen
Keine Tags, Fügen Sie den ersten Tag hinzu!
Beschreibung
Zusammenfassung:Hydroxy terminated polybutadiene is reacted with naphtyl-potassium and 1-bromo-2,4-pentadiene in successive steps to form a bis(1,3-pentadienyl ether) derivative. Then the bismaleimide of dimer diamine is added to the polybutadiene derivative whereby a room temperature cure to an elastomer is achieved.