Method for producing supported Raney nickel catalyst
A method for making a supported Raney nickel catalyst by coating a nickel substrate with aluminum or aluminum-nickel alloy, heat treating the coated substrate above the melting point of aluminum but below 1133 DEG C, quenching at a temperature below 854 DEG C to form NiAl3 as a solid phase in the su...
Gespeichert in:
Hauptverfasser: | , , , , , |
---|---|
Format: | Patent |
Sprache: | eng |
Schlagworte: | |
Online-Zugang: | Volltext bestellen |
Tags: |
Tag hinzufügen
Keine Tags, Fügen Sie den ersten Tag hinzu!
|
Zusammenfassung: | A method for making a supported Raney nickel catalyst by coating a nickel substrate with aluminum or aluminum-nickel alloy, heat treating the coated substrate above the melting point of aluminum but below 1133 DEG C, quenching at a temperature below 854 DEG C to form NiAl3 as a solid phase in the substrate. The Raney nickel alloy coating is activated in the usual manner by leaching with sodium hydroxide solution. |
---|