Direct-positive silver halide emulsion fogged to low level and the use thereof in energetic-surface development

Direct-positive silver halide emulsions are described which have been fogged so that a test portion thereof when coated at a coverage of 0.50 to 5.50 g of silver per sq.m. gives a density below 0.50 upon processing without exposure for 6 min. at 20 DEG C in a developer I and an identical coated test...

Ausführliche Beschreibung

Gespeichert in:
Bibliographische Detailangaben
Hauptverfasser: BORGINON, HENDRIK ALFONS, VANASSCHE, WILLY JOSEPH, PATTYN, HERMAN ALBERIK
Format: Patent
Sprache:eng
Schlagworte:
Online-Zugang:Volltext bestellen
Tags: Tag hinzufügen
Keine Tags, Fügen Sie den ersten Tag hinzu!
Beschreibung
Zusammenfassung:Direct-positive silver halide emulsions are described which have been fogged so that a test portion thereof when coated at a coverage of 0.50 to 5.50 g of silver per sq.m. gives a density below 0.50 upon processing without exposure for 6 min. at 20 DEG C in a developer I and an identical coated test portion gives a density that is at least twice that of the first test portion with a minimum of 0.50 upon processing without exposure for 3 min. at 20 DEG C in a developer II.