METHOD OF MAKING RIM-STABILIZED STEEL INGOTS

Rim-stabilized steel ingots are produced by teeming a rimming-type steel into an ingot mold until the ingot is about 80-95 percent full, whereupon teeming is interrupted to allow a rimming action in the mold for a period of from 1/2 to 15 minutes. Thereafter, teeming is continued until the mold is f...

Ausführliche Beschreibung

Gespeichert in:
Bibliographische Detailangaben
Hauptverfasser: OROSKI M,US, BALES J,US
Format: Patent
Sprache:eng
Schlagworte:
Online-Zugang:Volltext bestellen
Tags: Tag hinzufügen
Keine Tags, Fügen Sie den ersten Tag hinzu!
Beschreibung
Zusammenfassung:Rim-stabilized steel ingots are produced by teeming a rimming-type steel into an ingot mold until the ingot is about 80-95 percent full, whereupon teeming is interrupted to allow a rimming action in the mold for a period of from 1/2 to 15 minutes. Thereafter, teeming is continued until the mold is full. After teeming is commenced following the rimming action, sufficient molten aluminum is added to the mold to produce an SK steel within the rim, all of said aluminum being added prior to completion of the steel teeming.