Method of making a reconstituted tobacco sheet

1,165,454. Reconstituting tobacco. PHILIP MORRIS Inc. 23 May, 1967 [16 June, 1966], No. 23960/67. Heading A2C. Reconstituted tobacco sheet is made by reacting tobacco with an aqueous solution of a water-soluble orthophosphate at a temperature up to 300‹F. , using 1 to 30 parts by weight of the ortho...

Ausführliche Beschreibung

Gespeichert in:
Bibliographische Detailangaben
1. Verfasser: HIND JOHN D
Format: Patent
Sprache:eng
Schlagworte:
Online-Zugang:Volltext bestellen
Tags: Tag hinzufügen
Keine Tags, Fügen Sie den ersten Tag hinzu!
container_end_page
container_issue
container_start_page
container_title
container_volume
creator HIND JOHN D
description 1,165,454. Reconstituting tobacco. PHILIP MORRIS Inc. 23 May, 1967 [16 June, 1966], No. 23960/67. Heading A2C. Reconstituted tobacco sheet is made by reacting tobacco with an aqueous solution of a water-soluble orthophosphate at a temperature up to 300‹F. , using 1 to 30 parts by weight of the orthophosphate per 100 parts by weight of the tobacco; adding 1 to 50 parts by weight, per 100 parts by weight of the tobacco, of an alkaline earth metal phosphate; and casting the resultant material into a sheet. In the examples diammonium monohydrogen phosphate and calcium phosphate are used. Many other suitable alkaline earth metal phosphates are specified and include both synthetic and naturally occurring phosphates.
format Patent
fullrecord <record><control><sourceid>epo_EVB</sourceid><recordid>TN_cdi_epo_espacenet_US3386449A</recordid><sourceformat>XML</sourceformat><sourcesystem>PC</sourcesystem><sourcerecordid>US3386449A</sourcerecordid><originalsourceid>FETCH-epo_espacenet_US3386449A3</originalsourceid><addsrcrecordid>eNrjZNDzTS3JyE9RyE9TyE3MzsxLV0hUKEpNzs8rLsksKS1JTVEoyU9KTE7OVyjOSE0t4WFgTUvMKU7lhdLcDPJuriHOHrqpBfnxqcUFicmpeakl8aHBxsYWZiYmlo7GhFUAAEhiKdg</addsrcrecordid><sourcetype>Open Access Repository</sourcetype><iscdi>true</iscdi><recordtype>patent</recordtype></control><display><type>patent</type><title>Method of making a reconstituted tobacco sheet</title><source>esp@cenet</source><creator>HIND JOHN D</creator><creatorcontrib>HIND JOHN D</creatorcontrib><description>1,165,454. Reconstituting tobacco. PHILIP MORRIS Inc. 23 May, 1967 [16 June, 1966], No. 23960/67. Heading A2C. Reconstituted tobacco sheet is made by reacting tobacco with an aqueous solution of a water-soluble orthophosphate at a temperature up to 300‹F. , using 1 to 30 parts by weight of the orthophosphate per 100 parts by weight of the tobacco; adding 1 to 50 parts by weight, per 100 parts by weight of the tobacco, of an alkaline earth metal phosphate; and casting the resultant material into a sheet. In the examples diammonium monohydrogen phosphate and calcium phosphate are used. Many other suitable alkaline earth metal phosphates are specified and include both synthetic and naturally occurring phosphates.</description><language>eng</language><subject>CIGARETTES ; CIGARS ; HUMAN NECESSITIES ; MANUFACTURE OR PREPARATION OF TOBACCO FOR SMOKING ORCHEWING ; SMOKERS' REQUISITES ; SNUFF ; TOBACCO</subject><creationdate>1968</creationdate><oa>free_for_read</oa><woscitedreferencessubscribed>false</woscitedreferencessubscribed></display><links><openurl>$$Topenurl_article</openurl><openurlfulltext>$$Topenurlfull_article</openurlfulltext><thumbnail>$$Tsyndetics_thumb_exl</thumbnail><linktohtml>$$Uhttps://worldwide.espacenet.com/publicationDetails/biblio?FT=D&amp;date=19680604&amp;DB=EPODOC&amp;CC=US&amp;NR=3386449A$$EHTML$$P50$$Gepo$$Hfree_for_read</linktohtml><link.rule.ids>230,308,780,885,25555,76308</link.rule.ids><linktorsrc>$$Uhttps://worldwide.espacenet.com/publicationDetails/biblio?FT=D&amp;date=19680604&amp;DB=EPODOC&amp;CC=US&amp;NR=3386449A$$EView_record_in_European_Patent_Office$$FView_record_in_$$GEuropean_Patent_Office$$Hfree_for_read</linktorsrc></links><search><creatorcontrib>HIND JOHN D</creatorcontrib><title>Method of making a reconstituted tobacco sheet</title><description>1,165,454. Reconstituting tobacco. PHILIP MORRIS Inc. 23 May, 1967 [16 June, 1966], No. 23960/67. Heading A2C. Reconstituted tobacco sheet is made by reacting tobacco with an aqueous solution of a water-soluble orthophosphate at a temperature up to 300‹F. , using 1 to 30 parts by weight of the orthophosphate per 100 parts by weight of the tobacco; adding 1 to 50 parts by weight, per 100 parts by weight of the tobacco, of an alkaline earth metal phosphate; and casting the resultant material into a sheet. In the examples diammonium monohydrogen phosphate and calcium phosphate are used. Many other suitable alkaline earth metal phosphates are specified and include both synthetic and naturally occurring phosphates.</description><subject>CIGARETTES</subject><subject>CIGARS</subject><subject>HUMAN NECESSITIES</subject><subject>MANUFACTURE OR PREPARATION OF TOBACCO FOR SMOKING ORCHEWING</subject><subject>SMOKERS' REQUISITES</subject><subject>SNUFF</subject><subject>TOBACCO</subject><fulltext>true</fulltext><rsrctype>patent</rsrctype><creationdate>1968</creationdate><recordtype>patent</recordtype><sourceid>EVB</sourceid><recordid>eNrjZNDzTS3JyE9RyE9TyE3MzsxLV0hUKEpNzs8rLsksKS1JTVEoyU9KTE7OVyjOSE0t4WFgTUvMKU7lhdLcDPJuriHOHrqpBfnxqcUFicmpeakl8aHBxsYWZiYmlo7GhFUAAEhiKdg</recordid><startdate>19680604</startdate><enddate>19680604</enddate><creator>HIND JOHN D</creator><scope>EVB</scope></search><sort><creationdate>19680604</creationdate><title>Method of making a reconstituted tobacco sheet</title><author>HIND JOHN D</author></sort><facets><frbrtype>5</frbrtype><frbrgroupid>cdi_FETCH-epo_espacenet_US3386449A3</frbrgroupid><rsrctype>patents</rsrctype><prefilter>patents</prefilter><language>eng</language><creationdate>1968</creationdate><topic>CIGARETTES</topic><topic>CIGARS</topic><topic>HUMAN NECESSITIES</topic><topic>MANUFACTURE OR PREPARATION OF TOBACCO FOR SMOKING ORCHEWING</topic><topic>SMOKERS' REQUISITES</topic><topic>SNUFF</topic><topic>TOBACCO</topic><toplevel>online_resources</toplevel><creatorcontrib>HIND JOHN D</creatorcontrib><collection>esp@cenet</collection></facets><delivery><delcategory>Remote Search Resource</delcategory><fulltext>fulltext_linktorsrc</fulltext></delivery><addata><au>HIND JOHN D</au><format>patent</format><genre>patent</genre><ristype>GEN</ristype><title>Method of making a reconstituted tobacco sheet</title><date>1968-06-04</date><risdate>1968</risdate><abstract>1,165,454. Reconstituting tobacco. PHILIP MORRIS Inc. 23 May, 1967 [16 June, 1966], No. 23960/67. Heading A2C. Reconstituted tobacco sheet is made by reacting tobacco with an aqueous solution of a water-soluble orthophosphate at a temperature up to 300‹F. , using 1 to 30 parts by weight of the orthophosphate per 100 parts by weight of the tobacco; adding 1 to 50 parts by weight, per 100 parts by weight of the tobacco, of an alkaline earth metal phosphate; and casting the resultant material into a sheet. In the examples diammonium monohydrogen phosphate and calcium phosphate are used. Many other suitable alkaline earth metal phosphates are specified and include both synthetic and naturally occurring phosphates.</abstract><oa>free_for_read</oa></addata></record>
fulltext fulltext_linktorsrc
identifier
ispartof
issn
language eng
recordid cdi_epo_espacenet_US3386449A
source esp@cenet
subjects CIGARETTES
CIGARS
HUMAN NECESSITIES
MANUFACTURE OR PREPARATION OF TOBACCO FOR SMOKING ORCHEWING
SMOKERS' REQUISITES
SNUFF
TOBACCO
title Method of making a reconstituted tobacco sheet
url https://sfx.bib-bvb.de/sfx_tum?ctx_ver=Z39.88-2004&ctx_enc=info:ofi/enc:UTF-8&ctx_tim=2025-01-15T06%3A29%3A50IST&url_ver=Z39.88-2004&url_ctx_fmt=infofi/fmt:kev:mtx:ctx&rfr_id=info:sid/primo.exlibrisgroup.com:primo3-Article-epo_EVB&rft_val_fmt=info:ofi/fmt:kev:mtx:patent&rft.genre=patent&rft.au=HIND%20JOHN%20D&rft.date=1968-06-04&rft_id=info:doi/&rft_dat=%3Cepo_EVB%3EUS3386449A%3C/epo_EVB%3E%3Curl%3E%3C/url%3E&disable_directlink=true&sfx.directlink=off&sfx.report_link=0&rft_id=info:oai/&rft_id=info:pmid/&rfr_iscdi=true