COMPOSITE MATERIAL, THE METHOD OF ITS PREPARATION AND APPLICATION THEREOF

A stressed composite material is disclosed, characterized in that it contains Li4Ti5O12 spinel nanocrystallites in an amount of 25-93% by weight, encapsulated during the pyrolysis process in a tightly adherent and conductive carbon aerogel matrix with a carbon content of 7-74% by weight, with a spec...

Ausführliche Beschreibung

Gespeichert in:
Bibliographische Detailangaben
Hauptverfasser: KUBICKA, Marcelina, MOLENDA, Marcin, BAKIERSKA, Monika, CHUDZIK, Krystian, BIELEWSKI, Jakub
Format: Patent
Sprache:eng
Schlagworte:
Online-Zugang:Volltext bestellen
Tags: Tag hinzufügen
Keine Tags, Fügen Sie den ersten Tag hinzu!
Beschreibung
Zusammenfassung:A stressed composite material is disclosed, characterized in that it contains Li4Ti5O12 spinel nanocrystallites in an amount of 25-93% by weight, encapsulated during the pyrolysis process in a tightly adherent and conductive carbon aerogel matrix with a carbon content of 7-74% by weight, with a specific surface area of the composite of 44-426 m2/g, and a pore volume of the composite of 0.03-0.21 cm3/g, and an average pore size of the composite of 2-3 nm. Also disclosed is a method for obtaining the stressed composite material and an application of the stressed composite material for manufacturing electrode materials and lithium-ion cells.