PRODUCTION METHOD OF READY INJECTION MATERIAL INCLUDING NANO HYDRAULIC LIME

Clean version of the Abstract A production method of ready injection material aims at developing natural hydraulic lime at nano-size by using a single raw material. The production method includes: selecting marl, comprising at least 70% CaCO3, as the raw material, grinding the marl to have particle...

Ausführliche Beschreibung

Gespeichert in:
Bibliographische Detailangaben
Hauptverfasser: GUNER, Mehmet Bugra, HAZAR, Afife Binnaz, OKTAY, Didem, YUZER, Nabi, UGURYOL, Mehmet Fevzi
Format: Patent
Sprache:eng
Schlagworte:
Online-Zugang:Volltext bestellen
Tags: Tag hinzufügen
Keine Tags, Fügen Sie den ersten Tag hinzu!
Beschreibung
Zusammenfassung:Clean version of the Abstract A production method of ready injection material aims at developing natural hydraulic lime at nano-size by using a single raw material. The production method includes: selecting marl, comprising at least 70% CaCO3, as the raw material, grinding the marl to have particle size lower than 400 lam, calcining the marl at a temperature between 1000-1200° C., re-grinding the marl after the calcination process, reducing a d90 particle size of calcined marl to between 200-700 nm after the grinding process, applying a dry mixing process to the material having a reduced particle size, adding water to the material after dry mixing and applying mechanical mixing process during duration between 3-6 minutes at a revolution between 800-1000 rpm, adding super-fluidizing chemical additive to the obtained material, and mixing the material for duration between 3-6 minutes by using ultrasonic homogenizer and mechanic mixing.