HIGH-STRENGTH AL-CU-MG-MN ALUMINUM ALLOY AND PREPARATION METHOD THEREFOR

A high-strength Al-Cu-Mg-Mn aluminum alloy and a preparation method therefor is provided. The alloy includes the following components in percentage by weight: Si:≤0.5%, Fe: ≤0.5%, Cu: 4.5-6.3%, Mg: 0.6-1.2%, Mn: 0.6-1.5%, Sc: 0.15-0.35%, Zr: 0.1-0.2%, and Y: 0.1-0.3%, the balance being aluminum and...

Ausführliche Beschreibung

Gespeichert in:
Bibliographische Detailangaben
Hauptverfasser: LIU, Zuming, ZHOU, Xu, AI, Yongkang, LV, Xueqian, WEI, Bing, REN, Yake, NONG, Bizhong, LU, Sizhe, CAO, Bin
Format: Patent
Sprache:eng
Schlagworte:
Online-Zugang:Volltext bestellen
Tags: Tag hinzufügen
Keine Tags, Fügen Sie den ersten Tag hinzu!
Beschreibung
Zusammenfassung:A high-strength Al-Cu-Mg-Mn aluminum alloy and a preparation method therefor is provided. The alloy includes the following components in percentage by weight: Si:≤0.5%, Fe: ≤0.5%, Cu: 4.5-6.3%, Mg: 0.6-1.2%, Mn: 0.6-1.5%, Sc: 0.15-0.35%, Zr: 0.1-0.2%, and Y: 0.1-0.3%, the balance being aluminum and non-removable impurities. The preparation method includes: smelting, refining, impurity removing and degassing, pouring, homogenizing heat treatment, three-dimensional large deformation forging pre-deformation, isothermal deformation processing, and heat treatment. A casting mold used is a special combined mold having a metal mold as an inner mold, a surrounding cooling pipe, and a sand mold as an outer mold, and is used to prepare and obtain high-quality, high-performance castings. The heat treatment is solid solution treatment plus gradient aging treatment. The Al-Cu-Mg-Mn aluminum alloy has a tensile strength higher than 520 MPa and an elongation of 12-16%, that is, an increased elongation rate and improved strength.